A fiber membrane and hollow technology, which is applied in the field of preparation of end-type hollow fiber membranes, can solve the problems of disassembly and assembly, difficult cleaning, high price, and large waste of raw materials, so as to improve the application field and application range, and reduce maintenance and replacement costs. , the effect of improving production efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment 1
[0022] Specific embodiment 1, a method for preparing an end-type hollow fiber membrane, the steps are: the following components are calculated in parts by weight,
[0023] (1) Select polymer materials: 10 parts; additives: 1 part; mixed solvent: 60 parts; heat and dry the polymer materials and additives in an oven, and remove water from the mixed solvent through activated molecular sieves;
[0024] (2) Dissolving the polymer material and additives in the mixed solvent, then heating the mixture composed of the polymer material, additives and mixed solvent to a molten state, stirring to form a casting solution;
[0025] (3) Extrude the casting solution prepared in step (2) through a plum-blossom spinneret and enter it into the coagulation solution for cooling to undergo phase inversion. The fiber membrane after phase inversion undergoes post-treatment of pore preservation and air-dries at room temperature for 2 days Until the membrane is completely dry, thereby forming an end-ty...
specific Embodiment 2
[0028] Specific embodiment two, please refer to Figure 1-4 , a method for preparing an end-type hollow fiber membrane, the steps are: the following components are calculated in parts by weight,
[0029] (1), select polymer materials: 15 parts; additives: 6 parts; mixed solvent: 70 parts;
[0030] Heat and dry in the box, and the mixed solvent is dehydrated by activated molecular sieve;
[0031] (2) Dissolving the polymer material and additives in the mixed solvent, then heating the mixture composed of the polymer material, additives and mixed solvent to a molten state, stirring to form a casting solution;
[0032] (3) Extrude the casting solution prepared in step (2) through a plum-blossom spinneret and enter it into the coagulation solution for cooling to undergo phase inversion. The fiber membrane after phase inversion is post-treated to preserve pores, and air-dried at room temperature for 4 days Until the membrane is completely dry, thereby forming an end-type hollow fi...
specific Embodiment 3
[0036] Specific embodiment three: a kind of preparation method of end-type hollow fiber membrane, its step is: the following components are counted in parts by weight,
[0037] (1) Select polymer materials: 20 parts; additives: 10 parts; mixed solvent: 80 parts;
[0038] Heat and dry in the box, and the mixed solvent is dehydrated by activated molecular sieve;
[0039] (2) Dissolving the polymer material and additives in the mixed solvent, then heating the mixture composed of the polymer material, additives and mixed solvent to a molten state, stirring to form a casting solution;
[0040] (3) Extrude the casting solution prepared in step (2) through a plum-blossom spinneret and enter it into the coagulation solution to cool to undergo phase inversion. The fiber membrane after phase inversion is post-treated to preserve pores, and air-dried at room temperature for 5 days Until the membrane is completely dry, thereby forming an end-type hollow fiber membrane;
[0041]The polym...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com