Production method of weft-knitted double knitted polar fleece
A production method and technology of polar fleece, which are applied in the directions of weft knitting, knitting, textile material processing, etc., can solve the problems of poor napping effect of double-sided structure, and achieve a thick feel, good elasticity and good structural stability. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0041] A production method of weft-knitted double-sided knitted polar fleece, comprising the following steps:
[0042] S1 greige cloth preparation
[0043] S101, performing weaving processing on the gray cloth base material and the gray cloth raw material;
[0044] S102, drum washing machine, standard gear, water temperature 40°C, washing time 45 minutes;
[0045] S103, ring drying for about 2 hours;
[0046] S2 dyeing process
[0047] S201, cloth preparation: 24 hours for gray cloth loose cloth;
[0048] S202. Cooking and bleaching: Put 1% scouring enzyme, 1.5% hydrogen peroxide and 97.5% water in the dye vat, heat to 95°C, put the gray cloth in, the bath ratio of the gray cloth to the dye solution is 1:8, and the cooking and bleaching time is 30 minute;
[0049] S203, pre-pickling: put 1% glacial acetic acid in the dyeing vat and run for 10 minutes;
[0050] S204, dyeing and washing: put corresponding dyes and glacial acetic acid into the dyeing vat, and keep the tempe...
Embodiment 2
[0070] A production method of weft-knitted double-sided knitted polar fleece, comprising the following steps:
[0071] S1 greige cloth preparation
[0072] S101, weaving the gray cloth base material and the gray cloth raw material;
[0073] S102, drum washing machine, standard gear, water temperature 40°C, washing time 45 minutes;
[0074] S103, ring drying for about 2 hours;
[0075] S2 dyeing process
[0076] S201, cloth preparation: 24 hours for gray cloth loose cloth;
[0077] S202. Cooking and bleaching: Put 1% scouring enzyme, 1.5% hydrogen peroxide and 97.5% water in the dye vat, heat to 95°C, put the gray cloth in, the bath ratio of the gray cloth to the dye solution is 1:8, and the cooking and bleaching time is 30 minute;
[0078] S203, pre-pickling: put 1% glacial acetic acid in the dyeing vat and run for 10 minutes;
[0079] S204, dyeing and washing: put corresponding dyes and glacial acetic acid into the dyeing vat, and keep the temperature at 135°C for 60 minu...
Embodiment 3
[0099] A production method of weft-knitted double-sided knitted polar fleece, comprising the following steps:
[0100] S1 greige cloth preparation
[0101] S101, weaving the gray cloth base material and the gray cloth raw material;
[0102] S102, drum washing machine, standard gear, water temperature 40°C, washing time 45 minutes;
[0103] S103, ring drying for about 2 hours;
[0104] S2 dyeing process
[0105] S201, cloth preparation: 24 hours for gray cloth loose cloth;
[0106] S202. Cooking and bleaching: Put 1% scouring enzyme, 1.5% hydrogen peroxide and 97.5% water in the dye vat, heat to 95°C, put the gray cloth in, the bath ratio of the gray cloth to the dye solution is 1:8, and the cooking and bleaching time is 30 minute;
[0107] S203, pre-pickling: put 1% glacial acetic acid in the dyeing vat and run for 10 minutes;
[0108] S204, dyeing and washing: put corresponding dyes and glacial acetic acid into the dyeing vat, and keep the temperature at 135°C for 60 mi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology