Nonstick coating containing graphene material, and preparation method thereof
A non-stick pan and graphene technology, applied in coatings, special materials for cooking utensils, kitchen utensils, etc., can solve problems such as poor high temperature resistance and wear resistance, achieve excellent high temperature resistance, enhance over-temperature prompting effect, and enhance transmission The effect of thermal effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0050] Correspondingly, a kind of preparation method with the non-stick coating of graphene material as above, it may further comprise the steps:
[0051] S1. Sand blast the inner surface of the non-stick pan body, and its surface roughness is Ra2.8-3.5;
[0052] S2. After sequentially performing alkali washing, pickling and hot water washing operations on the inner surface of the non-stick pan body, dry it for later use;
[0053] S3. Mix 50-90 parts of polytetrafluoroethylene / polysulfone blend, 0.5-2 parts of modified graphene oxide, 1-5 parts of thermochromic pigments, 0.8-1.2 parts of modified silicon carbide whiskers, 1.5- 3 parts of additives and 15 to 35 parts of deionized water are stirred and mixed evenly, and then evenly coated on the non-stick pan body after surface treatment to form the bottom layer structure of the non-stick pan coating. The thickness of the bottom layer is 10 ~ 15um;
[0054] S4. Mix 35-75 parts of polytetrafluoroethylene resin, 1.5-5 parts of m...
Embodiment 1
[0060] A kind of non-stick pan coating with graphene material, described non-stick pan coating is made of bottom layer and surface layer; Described bottom layer is made up of the raw material of following parts by weight: 70 parts of polytetrafluoroethylene / polysulfone blend 1.5 parts of modified graphene oxide, 3 parts of thermochromic pigments, 1.1 parts of modified silicon carbide whiskers, 2.7 parts of additives and 25 parts of deionized water; the surface layer is composed of the following raw materials in parts by weight: 55 parts Parts of polytetrafluoroethylene resin, 3.5 parts of modified calcium carbonate whiskers, 5.4 parts of fatty alcohol polyoxyethylene ether ammonium sulfate, 7.2 parts of maleic anhydride and 48 parts of deionized water. The thickness of the bottom layer is 12um, and the thickness of the surface layer is 10um.
[0061] The mass ratio of polytetrafluoroethylene and polysulfone is 1:1.3. The polysulfone is polyethersulfone.
[0062] The preparat...
Embodiment 2
[0067] A kind of non-stick pan coating with graphene material, described non-stick pan coating is made of bottom layer and surface layer; Described bottom layer is made up of the raw material of following parts by weight: 50 parts of polytetrafluoroethylene / polysulfone blend 0.5 parts of modified graphene oxide, 1 part of thermochromic pigments, 0.8 parts of modified silicon carbide whiskers, 1.5 parts of additives and 15 parts of deionized water; the surface layer is composed of the following raw materials in parts by weight: 35 Parts of polytetrafluoroethylene resin, 1.5 parts of modified calcium carbonate whiskers, 3 parts of fatty alcohol polyoxyethylene ether ammonium sulfate, 5 parts of maleic anhydride and 35 parts of deionized water. The thickness of the bottom layer is 10um, and the thickness of the surface layer is 8um.
[0068] The mass ratio of polytetrafluoroethylene and polysulfone is 1:1.2. The polysulfone is polyethersulfone.
[0069] The preparation method o...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com