[0034] Mix chitosan, EVA emulsion and polyvinylidene fluoride, and stir to obtain the main resin; take organic montmorillonite, aluminum trichloride, and deionized water, mix organic montmorillonite and deionized water, and ultrasonically disperse. That is to get the suspension, add aluminum trichloride to the suspension, place it in a ball mill, and ball mill it to get the mixed slurry; filter the mixed slurry to get the precipitate, wash and dry the precipitate, cool to room temperature, and grind After sieving, the filler can be obtained; take the main resin, filler, hydroxycellulose ether, pigment and filler titanium dioxide, dispersant polyethylene glycol 200, lubricant silicone oil, polysiloxane defoamer, antifungal agent Z-101 , deionized water, mix hydroxycellulose ether, pigment and filler titanium dioxide, dispersant polyethylene glycol 200, lubricant silicone oil, polysiloxane defoamer, antifungal agent Z-101 and deionized water, stir at high speed After processing,...
Embodiment 2
[0036] Mix chitosan, EVA emulsion and polyvinylidene fluoride, and stir to obtain the main resin; take organic montmorillonite, aluminum trichloride, and deionized water, mix organic montmorillonite and deionized water, and ultrasonically disperse. That is to get the suspension, add aluminum trichloride to the suspension, place it in a ball mill, and ball mill it to get the mixed slurry; filter the mixed slurry to get the precipitate, wash and dry the precipitate, cool to room temperature, and grind After sieving, the filler can be obtained; take the main resin, filler, hydroxycellulose ether, pigment and filler titanium dioxide, dispersant polyethylene glycol 200, lubricant silicone oil, polysiloxane defoamer, antifungal agent Z-101 , deionized water, mix hydroxycellulose ether, pigment and filler titanium dioxide, dispersant polyethylene glycol 200, lubricant silicone oil, polysiloxane defoamer, antifungal agent Z-101 and deionized water, stir at high speed After processing,...
Embodiment 3
[0038] Mix chitosan, EVA emulsion and polyvinylidene fluoride, and stir to obtain the main resin; take organic montmorillonite, aluminum trichloride, and deionized water, mix organic montmorillonite and deionized water, and ultrasonically disperse. That is to get the suspension, add aluminum trichloride to the suspension, place it in a ball mill, and ball mill it to get the mixed slurry; filter the mixed slurry to get the precipitate, wash and dry the precipitate, cool to room temperature, and grind After sieving, the filler can be obtained; take the main resin, filler, hydroxycellulose ether, pigment and filler titanium dioxide, dispersant polyethylene glycol 200, lubricant silicone oil, polysiloxane defoamer, antifungal agent Z-101 , deionized water, mix hydroxycellulose ether, pigment and filler titanium dioxide, dispersant polyethylene glycol 200, lubricant silicone oil, polysiloxane defoamer, antifungal agent Z-101 and deionized water, stir at high speed After processing,...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com