A harmless resource treatment method for medical waste
A medical waste and treatment method technology, applied in the field of waste utilization, can solve the problems of biological pollution in the storage environment of medical waste, low burnout rate, cross-infection in hospitals, etc. The effect of harmful diseases
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] Harmless resource treatment method for medical waste, including the following steps: (1) After mixing the medical waste and calcium oxide by mass 1: 0.12, 130 ° C dry, smash to 150 mesh; (2) 30 parts of the pulverization of step 1, 15 parts of corrosion, calcination zeolite, 3 copies of iron carbonyl, 3 methacmide, 70 cement clinkers, 15 copies of the cement material, mix well, add a total amount of 25% water, add total amount of 25% water. After stirring, solidification is solid; the corrosion calcined zeolite is submerged by zeolite in concentrated hydrochloric acid for 15 minutes after calcination; (3) Put the cured material obtained by step (2) at 700 ° C, high temperature, After calcination at a nitrogen range. The cementing material is a commercially available gypsum.
Embodiment 2
[0024] A harmless resource treatment method for medical waste, including the following steps: (1) After mixing medical waste and calcium oxide by mass, 140 ° C dry after 140 ° C, crushing to 100 mesh; (2) 40 parts of the pulverization of step 1, 10 corrosion calcined zeolite, 4 parts of the five carbonyl, 2 parts of methylphosphatamide, 80 cement clinkers, 10 colloidal materials, mix well, add 30% water, add 30% water. After stirring, curing is formed; the corrosion calcined zeolite is soaked with zeolite for 10 minutes, and then calcined after calcination at 400 ° C. The cured material obtained in step (2) is 600 ° C high temperature, After calcination at a nitrogen range. The cementing material is a commercially available gypsum.
Embodiment 3
[0026] Harmless resource treatment method for medical waste, including the following steps: (1) After mixing medical waste and calcium oxide by mass 1: 0.14, 120 ° C dry after 120 ° C, pulverize to 200 mesh; (2) 20 parts of the pulverization of step 1, 20 parts of corrosion, 2 copies of zeolite, 4 methacarbonate, 4 parts of methylphosphatamide, 60 cement clinkers, 20 copies of the cement material, mix well, add the total amount of 20% water, add the total amount of 20% water. After stirring, solidification is solid; the corrosion calcined zeolite is soaked with zeolite for 20 minutes, and then calcined after calcination at 300 ° C .; (3) Put the cured material obtained by step (2) at 800 ° C high temperature, After calcination at a nitrogen range. The cementing material is a commercially available gypsum.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com