Embodiment 1
[0055] A filter material for an aquarium system, the preparation method of the filter material is as follows:
[0056] 1) Immerse the activated carbon into the metal salt solution sequentially at a temperature of 30°C. The immersion time of each metal salt solution is 2 hours, dry at 120°C, and repeatedly immerse until the solution is completely absorbed.
[0057] 2) The activated carbon that has completely absorbed the metal salt solution was calcined at 500° C. for 4 hours under the condition of isolation from air, and cooled naturally to room temperature.
[0058] 3) Impregnate the calcined activated carbon in the aqueous solution of the catalyst and the acidifying agent in sequence at 30°C. The immersion time of each aqueous solution is 2 hours, dry at 120°C, and repeatedly impregnate until the solution is completely absorbed.
[0059] The ratio of metal salt, catalyst and acidifying agent supported on activated carbon is: 50:15:10.
[0060] in,
[0061] The metal salts ...
Embodiment 2
[0065] A filter material for an aquarium system, the preparation method of the filter material is as follows:
[0066] 1) Immerse the activated carbon into the metal salt solution sequentially at a temperature of 30°C. The immersion time of each metal salt solution is 2 hours, dry at 120°C, and repeatedly immerse until the solution is completely absorbed.
[0067] 2) The activated carbon that has completely absorbed the metal salt solution was calcined at 500° C. for 4 hours under the condition of isolation from air, and cooled naturally to room temperature.
[0068] 3) Impregnate the calcined activated carbon in the aqueous solution of the catalyst and the acidifying agent in sequence at 30°C. The immersion time of each aqueous solution is 2 hours, dry at 120°C, and repeatedly impregnate until the solution is completely absorbed.
[0069] The ratio of metal salt, catalyst and acidifying agent supported on activated carbon is: 50:10:15.
[0070] in,
[0071] The metal salts ...
Embodiment 3
[0075] A filter material for an aquarium system, the filter material is composed of the following components:
[0076] 40% activated carbon, 30% iron salt, 10% aluminum salt, 3% copper salt, 5% binder, 5% catalyst, 7% acidifier with slow release function.
[0077] in,
[0078] Binder: a mixture of polyvinyl alcohol and sodium carboxymethyl cellulose in a mass ratio of 1:1;
[0079] Catalyst: a mixture of calcium peroxide, calcium oxide, and silicon dioxide in a mass ratio of 1:0.5:0.2
[0080] Acidifying agent with slow-release function: phosphoric acid, citric acid, and lactic acid are mixed in a mass ratio of 1:1:1, then mixed with silicon dioxide, and embedded in a slow-release material. The mass ratio of silicon oxide and slow-release material is 1:0.5:0.8, and the slow-release material is a mixture of shellac and magnesium stearate in a mass ratio of 1:1.
[0081] The preparation method of this filter material is as follows:
[0082] 1) Immerse the activated carbon in...
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com