High polymer composite material
A composite material and polymer technology, applied in the field of polymer composite materials, can solve problems such as difficult to apply to families, affect light, poor shading performance, etc., achieve good UV discoloration performance, improve protection performance, and good UV protection. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0031] The preparation method of polyethylene terephthalate modified photochromic agent comprises the following steps:
[0032] 1) Add terephthalic acid and ethylene glycol into the reactor, heat the reactor and stir it to carry out esterification reaction, generate esterification product, and cool to solid; the reaction temperature is 180-220°C; the reaction time is 1 -4 hours.
[0033] 2) Grinding the esterification product into powder to obtain the esterification product powder;
[0034] 3) The powder of the esterification product and the inorganic color-changing agent are fully mixed and then subjected to vacuum polycondensation reaction to prepare a polyethylene terephthalate modified photochromic agent. When the vacuum polycondensation reaction is carried out, the vacuum is kept stable in this application, and the polycondensation conditions of low vacuum in the early stage and high vacuum in the late stage cannot be used in some existing technologies.
[0035] In this...
Embodiment 1
[0038] A polymer composite material comprising at least photochromic fibers;
[0039] Photochromic fiber by weight, it consists of:
[0040]
[0041] The inorganic photochromic agent among them is CaHfO3: La 2 o 3 .
[0042] In the polymethyl methacrylate modified photochromic agent, the photochromic agent accounts for 3% of the total weight of the polymethyl methacrylate modified photochromic agent.
[0043] The auxiliary agent includes one or more combinations of oxidizing agent, compatibilizer, antiaging agent and light stabilizer.
[0044] The preparation method of polyethylene terephthalate modified photochromic agent comprises the following steps:
[0045] 1) Add terephthalic acid and ethylene glycol to the reactor, the reaction temperature is 180°C; the reaction time is 1 hour, the reactor is heated and stirred to carry out the esterification reaction, and the esterification product is formed, and cooled to a solid;
[0046] 2) Grinding the esterification produc...
Embodiment 2
[0049] A polymer composite material comprising at least photochromic fibers;
[0050] Photochromic fiber by weight, it consists of:
[0051]
[0052] The inorganic photochromic agent among them is CaHfO3: La 2 o 3 .
[0053] In the polymethyl methacrylate modified photochromic agent, the photochromic agent accounts for 5% of the total weight of the polymethyl methacrylate modified photochromic agent.
[0054] The auxiliary agent includes one or more combinations of oxidizing agent, compatibilizer, antiaging agent and light stabilizer.
[0055]The preparation method of polyethylene terephthalate modified photochromic agent comprises the following steps:
[0056] 1) Add terephthalic acid and ethylene glycol to the reactor, the reaction temperature is 220°C; the reaction time is 4 hours, the reactor is heated and stirred, and the esterification reaction is carried out to generate an esterified product, which is cooled to a solid;
[0057] 2) Grinding the esterification pr...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com