A coal-saving agent and emulsifier technology, applied in the field of energy conservation and environmental protection, can solve the problems of easy volatility, high cost of raw materials, complex process, etc., and achieve the effects of reducing emissions, increasing load capacity, and improving combustion efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] A preparation method of a coal-saving agent, comprising the following steps:
[0029] (1) Diatomite and chitosan solution with a mass concentration of 2% are mixed according to a weight ratio of 1:25, and ultrasonically vibrated at a frequency of 60HZ for 20min to obtain a dispersion;
[0030] (2) Add tetrabutyl titanate to the above dispersion, then raise the temperature to 35°C and ultrasonically disperse for 50 minutes, let it stand for 1 hour, filter to obtain the filter residue, and dry the filter residue at 100°C to obtain the modified chitosan diatomite;
[0031] (3) Put 2 parts by weight of sodium hydroxide, 6 parts by weight of manganese dioxide, and 5 parts by weight of potassium permanganate into 15 parts by weight of saturated lime water, stir evenly, then add 2 parts by weight of ammonium nitrate and 3 parts by weight of bicarbonate ammonium, mixed uniformly to obtain a mixed solution;
[0032] (4) Adding an alkylphenol polyoxyethylene ether emulsifier to...
Embodiment 2
[0036] A preparation method of a coal-saving agent, comprising the following steps:
[0037] (1) Diatomaceous earth and chitosan solution with a mass concentration of 1.5% were mixed according to a weight ratio of 2:33, and ultrasonically oscillated at a frequency of 60HZ for 25min to obtain a dispersion;
[0038] (2) Add tetrabutyl titanate to the above dispersion liquid, then raise the temperature to 40°C and ultrasonically disperse for 45min, let stand for 1h, filter to obtain filter residue, dry the filter residue at 100°C to obtain modified chitosan diatomite;
[0039] (3) Put 2 parts by weight of sodium hydroxide, 7 parts by weight of manganese dioxide, and 5 parts by weight of potassium permanganate into 20 parts by weight of saturated lime water, stir evenly, then add 2 parts by weight of ammonium nitrate and 5 parts by weight of bicarbonate ammonium, mixed uniformly to obtain a mixed solution;
[0040] (4) Add a sulfonic acid lipid emulsifier to the above mixed solu...
Embodiment 3
[0044]A preparation method of a coal-saving agent, comprising the following steps:
[0045] (1) Diatomite and chitosan solution with a mass concentration of 2% are mixed according to a weight ratio of 1:30, and ultrasonically oscillated at a frequency of 50HZ for 20min to obtain a dispersion;
[0046] (2) Add tetrabutyl titanate to the above dispersion liquid, then heat up to 38°C and disperse ultrasonically for 50 minutes, let stand for 2 hours, filter to obtain filter residue, dry the filter residue at 100°C to obtain modified chitosan diatomite;
[0047] (3) 1 part by weight of sodium hydroxide, 6 parts by weight of manganese dioxide, and 4 parts by weight of potassium permanganate are put into 15 parts by weight of saturated lime water, stir evenly, then add 3 parts by weight of ammonium nitrate and 3 parts by weight of bicarbonate ammonium, mixed uniformly to obtain a mixed solution;
[0048] (4) Add a fatty polyoxyethylene emulsifier to the above mixed solution, contro...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com