A technology of cleaborol and sustained-release film, applied in the field of biomedical materials, can solve the problems of not being able to be retained for a long time, easy to be wiped, etc., to achieve the effect of enhancing drug penetration ability, treating fungal infection, and strong penetration ability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0027] A, the first layer of sustained-release film preparation: with crisborole 20%, glycerin 25%, microcrystalline cellulose 25%, absorption enhancer 7% (wherein propylene glycol 60%, polysorbate 10%, menthol 10% , grass fruit oil 10% and clove oil 10%), carrageenan 8%, polyvinylpyrrolidone 15% mix fully, melt, extrude film-forming agent with extruder;
[0028] B, the preparation of the second layer of delayed-release film: with crisborole 20%, propylene alcohol 25%, sorbitol 25%, absorption accelerator 7% (propylene glycol 60%, polysorbate 10%, menthol 10%, Straw fruit oil 10% and clove oil 10%), guar gum 8%, polycarbophil 15% mix fully, add appropriate amount of water to dissolve, stir evenly, apply it evenly on the above-mentioned slow-release film, dry in a dryer Dry until there is no obvious moisture, and the drying temperature is 60°C;
[0029] C. Cut and get.
Embodiment 2
[0031] A, the first layer of sustained-release film preparation: with crisborole 25%, polyethylene glycol 23%, modified starch 22%, absorption accelerator 8% (propylene glycol 60%, polysorbate 10%, menthol 10%) , grass fruit oil 10% and clove oil 10%), sodium carboxymethyl cellulose 7%, chitosan 15% mix fully, melt, extrude film-forming agent with extruder;
[0032] B, the second layer of delayed-release film preparation: with crisborole 25%, triacetin 23%, dextrin 22%, absorption enhancer 8% (propylene glycol 60%, polysorbate 10%, menthol 10%) , grass fruit oil 10% and clove oil 10%), sodium carboxymethyl cellulose 7%, polyvinyl alcohol 15% mix well, add appropriate amount of water to dissolve, stir well, apply it evenly on the above-mentioned slow-release film, bake Dry in a dryer until there is no obvious moisture, and the drying temperature is 60°C;
[0033] C. Cut and get.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com