Rust-proof treatment liquid and preparation method thereof
A technology of antirust treatment and phthalimidovaleric acid, applied in the petroleum industry, lubricating compositions, etc., can solve the problems of high toxicity, environmental pollution, etc., achieve low cost, high anticorrosion efficiency, increase anticorrosion The effect of the rust effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] A kind of antirust treatment liquid, its raw material comprises by weight: 9 parts of phthalimido valeric acid, 6 parts of citric acid, 5 parts of tetrabutyl acetic acid, 5 parts of phytic acid, 20 parts of pentaerythritol, 5 parts of sodium molybdate, 0.5 part of polyoxyethylene polyoxypropylene pentaerythritol ether, 0.4 part of fatty acid glyceride, 55 parts of water.
Embodiment 2
[0018] A kind of antirust treatment liquid, its raw material comprises by weight: 18 parts of phthalimido valeric acid, 12 parts of citric acid, 10 parts of tetrabutyl acetic acid, 10 parts of phytic acid, 30 parts of pentaerythritol, 10 parts of sodium molybdate, 1 part of polydimethylsiloxane, 1 part of stearic acid, 70 parts of water.
Embodiment 3
[0020] A kind of antirust treatment liquid, 12 parts of phthalimido valeric acid, 8 parts of citric acid, 6 parts of tetrabutyl acetic acid, 6 parts of phytic acid, 24 parts of pentaerythritol, 7 parts of sodium molybdate, poly 0.6 part of oxyethylene polyoxypropylene pentaerythritol ether, 0.5 part of fatty acid glyceride, and 60 parts of water.
[0021] The preparation method of the above-mentioned antirust treatment liquid comprises the following steps: uniformly mixing phthalimidovaleric acid, citric acid, tetrabutylacetic acid, phytic acid, pentaerythritol and toluene, and reacting at reflux for 5 hours at a temperature of 80°C Finally, toluene and water were removed to obtain preform A; preform A, sodium molybdate, polyoxyethylene polyoxypropylene pentaerythritol ether, fatty acid glyceride and water were stirred at a speed of 150 rpm for 3 hours at a temperature of 70°C to prepare Anti-rust treatment fluid.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com