Looking for breakthrough ideas for innovation challenges? Try Patsnap Eureka!

Supported hydrochloric acid decolorizing agent as well as preparation method and decolorization process thereof

A supported reagent and decolorizing agent technology, applied in chemical instruments and methods, halogen/halogen acid, chlorine/hydrogen chloride purification, etc., can solve the problems of difficult resin handling, waste of resources, environmental pollution, etc., and achieve short production cycle and effect. Good, short depigmentation time

Inactive Publication Date: 2018-08-10
CHINA THREE GORGES UNIV
View PDF8 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

At present, hydrochloric acid is decolorized and impurity-removed, and the method of producing refined hydrochloric acid is mainly to process industrial hydrochloric acid with various resins, and the cost is higher in this process, and the processed resin is more difficult to handle, causing environmental pollution and waste of resources

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0019] The components of the novel load-type reagent used for hydrochloric acid decolorization are by weight percentage: 10% MCM-41 treated with trimethoxysilylpropylamine and trimethylchlorosilane (the specific treatment process is: 20 grams of trimethyl Oxysilyl propylamine is dissolved in 160 milliliters of anhydrous dichloromethane, and this solution is added in the suspension of the anhydrous chloroform that contains 28 grams of ordered mesoporous material MCM-41 of 1600 milliliters.The mixture is at 65 ℃ Stirring for 24 hours. The solid was then filtered and washed with dichloromethane (2*200 mL), and dried under vacuum at 160 °C for 5 hours. The dried solid was then added to 1000 mL of anhydrous chloroform, and 50 g of Tris Chloromethylsilane, stirred at room temperature for 24 hours. Then filtered to obtain a solid powder, which was washed with acetone (3*200 ml) and ether (3*200 ml), and dried in vacuum at 120 ° C for 5 hours to obtain The above-mentioned ordered meso...

Embodiment 2

[0021] The components of the novel load-type reagent used for hydrochloric acid decolorization are by weight percentage: 20% MCM-41 treated with trimethoxysilylpropylamine and trimethylchlorosilane (the specific treatment process is: 20 grams of trimethyl Oxysilyl propylamine is dissolved in 160 milliliters of anhydrous dichloromethane, and this solution is added in the suspension of the anhydrous chloroform that contains 28 grams of ordered mesoporous material MCM-41 of 1600 milliliters.The mixture is at 65 ℃ Stirring for 24 hours. The solid was then filtered and washed with dichloromethane (2*200 mL), and dried under vacuum at 160 °C for 5 hours. The dried solid was then added to 1000 mL of anhydrous chloroform, and 50 g of Tris Chloromethylsilane, stirred at room temperature for 24 hours. Then filtered to obtain a solid powder, which was washed with acetone (3*200 ml) and ether (3*200 ml), and dried in vacuum at 120 ° C for 5 hours to obtain The above-mentioned ordered meso...

Embodiment 3

[0023] The components of the novel load-type reagent used for hydrochloric acid decolorization are by weight percentage: 20% MCM-41 treated with trimethoxysilylpropylamine and trimethylchlorosilane (the specific treatment process is: 20 grams of trimethyl Oxysilyl propylamine is dissolved in 160 milliliters of anhydrous dichloromethane, and this solution is added in the suspension of the anhydrous chloroform that contains 28 grams of ordered mesoporous material MCM-41 of 1600 milliliters.The mixture is at 65 ℃ Stirring for 24 hours. The solid was then filtered and washed with dichloromethane (2*200 mL), and dried under vacuum at 160 °C for 5 hours. The dried solid was then added to 1000 mL of anhydrous chloroform, and 50 g of Tris Chloromethylsilane, stirred at room temperature for 24 hours. Then filtered to obtain a solid powder, which was washed with acetone (3*200 ml) and ether (3*200 ml), and dried in vacuum at 120 ° C for 5 hours to obtain The above-mentioned ordered meso...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention relates to a novel supported hydrochloric acid decolorizing agent as well as a preparation method and a decolorization process thereof. The decolorizing agent can be used for quite effectively removing the color of industrial hydrochloric acid; the decolorized industrial hydrochloric acid is colorless transparent liquid. A reagent is prepared from an ordered mesoporous material MCM-41 (the MCM-41 treated through trimethoxysilyl propylamine and trimethylchlorosilane), 2-p-bromomethyl bipyridine, sulfurous acid, ferrous chloride, magnesium sulfate, stannous chloride, diatomite, water and ethanol. The reagent capable of being used for decolorizing hydrochloric acid, which is provided by the invention, is simple in preparation process, short in production period and low in cost,is used for decolorizing the industrial hydrochloric acid, is short in decolorization time and good in decolorization effect, and does not decrease the content of the industrial hydrochloric acid, andthe decolorizing agent can be repeatedly recovered and utilized for multiple times.

Description

technical field [0001] The invention relates to the technical field of fine chemicals, in particular to a novel load-type hydrochloric acid decolorizer, a preparation method and a decolorization process thereof. Background technique [0002] In recent years, a large amount of by-product hydrochloric acid is produced every year in the fine chemical industry, for example, a large amount of hydrochloric acid is produced in the process of preparing compound fertilizer. Because hydrochloric acid has strong corrosiveness, it will seriously corrode iron pipelines and other equipment, resulting in the production and preparation of industrial hydrochloric acid containing a large amount of ferric ions, which makes the hydrochloric acid yellow. At the same time, in the process of compound fertilizer by-product hydrochloric acid, due to the impurity of the raw materials for the preparation of compound fertilizer, the produced hydrochloric acid will contain a large amount of bromine mole...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
IPC IPC(8): C01B7/07
CPCC01B7/0706
Inventor 王龙刘明国刘杨黄年玉李德江
Owner CHINA THREE GORGES UNIV
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products