A translucent and polyurethane technology, applied in polyurea/polyurethane coatings, coatings, etc., can solve problems such as fingerprints are not easy to disappear, furniture has peculiar smell, heavy metals exceed the standard, etc., and achieve the effects of improving scratch resistance, not easy to sag, and low toxicity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] According to the formula weight ratio, add 21.5 parts of mixed solvent into the dispersing tank, add 50 parts of 70% solid-containing alkyd resin, add 8 parts of DISPERBYK-180 color paste dispersant and stir evenly, slowly add 20 parts of translucent chestnut red calcined Amba powder, 0.2 part of defoamer, 0.3 part of anti-sedimentation agent, and then disperse at a high speed of 1000-1200r / min for 45-60 minutes, and then go to the horizontal sand mill to grind 5-8 times until the fineness of the color paste When the particle size reaches the requirement of ≤5μ, it is transferred to the paint mixing tank for defoaming and viscosity adjustment, and is filtered and packaged to obtain millet red color paste.
Embodiment 2
[0026] According to the formula weight ratio, add 18.8 parts of mixed solvent into the dispersion tank, add 60 parts of 70% solid-containing alkyd resin, stir evenly, add 4 parts of matting powder, 0.5 parts of dispersant, disperse at high speed for 30-40 minutes, and disperse at low speed Add 15 parts of chestnut red color paste, 0.3 parts of titanate-modified silicone chelating leveling agent, 0.2 parts of fluorine-modified acrylic leveling agent, 0.2 parts of modified silicone defoamer, and 1 part of anti-settling agent under stirring. After stirring and passing the test, it was filtered and packaged to obtain the first component of translucent chestnut red calcined amba net odor type polyurethane wood lacquer.
Embodiment 3
[0028] Add 40 parts of TDI / TMP adduct, 30 parts of HDI trimer, and 30 parts of mixed solvent into the dispersion tank and stir evenly. After passing the test, filter and pack to obtain translucent chestnut red calcined amba net odor type polyurethane wood paint. B component.
[0029] Mix the paint according to the ratio of component A: component B = 1:0.5, and add thinner to adjust the viscosity to spray or brush.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com