Three-dimensional patterned slip-proof gloves and preparation process thereof
A technology of three-dimensional pattern and preparation process, which is applied in the field of latex gloves, can solve problems such as unbalanced patterns, troublesome pairing of left and right hands, inconsistent patterns, etc., and achieve enhanced anti-slip effects, enhanced grip effects, and balanced coating patterns
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0021] A kind of three-dimensional pattern anti-slip gloves, the raw material of described anti-slip gloves comprises following components by weight part: 28 parts of prevulcanized natural rubber latex, 5 parts of sodium carboxymethyl cellulose (CMC), 6 parts of colloidal calcium carbonate, emulsifier 1 part, also includes potassium hydroxide, and the added amount of potassium hydroxide is 100g-375g based on 200kg of the above-mentioned total amount of raw materials.
[0022] The raw materials of the pre-vulcanized natural rubber latex include the following components: natural rubber latex, vulcanizing agent, accelerator, emulsifier, and anti-aging agent. The mass percent concentration of the sodium carboxymethylcellulose in water is 9%.
[0023] The present invention also provides a preparation process of three-dimensional pattern anti-skid gloves, comprising the following steps:
[0024] (1) Preparation of pre-vulcanized natural rubber latex: get natural rubber latex, vulca...
Embodiment 2
[0030] Design four groups of experiments, be respectively experimental group 1, experimental group 2, control group 1, control group 2, four groups of experiments are all prepared according to the preparation process described in above-mentioned embodiment 1, only change the amount of potassium hydroxide in the raw material, other The raw material components are identical (based on the 200kg raw material total amount), and the experimental results obtained are as shown in table 1:
[0031] Table 1: Effect of potassium hydroxide addition on coating pattern
[0032]
[0033] The above experimental results show that when the amount of potassium hydroxide added is in the range of 100g-375g, better patterns and three-dimensional effects can be obtained, such as figure 2 and image 3 As shown; the addition of potassium hydroxide is too small, the pattern is small, flat, and the three-dimensional effect is poor, such as figure 1 As shown; when the addition of potassium hydroxi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com