Waterborne two-component quick-drying polymer cement waterproof mortar
A quick-drying, waterproof mortar technology, used in the field of building waterproofing, can solve problems such as sagging corners and cracks, and achieve the effects of good water and alkali resistance, good weather resistance, high bonding strength, and good impermeability.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0063] A water-based two-component quick-drying polymer cement waterproof mortar, including powder and liquid, wherein the powder is composed of the following components: Portland cement 40%, sulfoaluminum cement 12%, microcrystalline powder 13% , Quartz sand 34.05%, high-strength anti-cracking fiber 0.38%, water-retaining agent 0.02%, powder defoamer 0.1%, water-reducing agent 0.1%, retarder 0.05%, early-strength agent 0.1%, water-repellent agent 0.2%; The liquid material is composed of the following components: 37% polymer emulsion, 0.15% liquid defoamer, 0.25% preservative, 0.1% pH regulator, and water as the balance.
[0064] The mixing ratio of the above-mentioned powder material and liquid material is 2.5:1 by weight.
[0065] Among them, Portland cement is PII42.5 Portland cement; sulfoaluminum cement is low alkalinity sulfoaluminate cement with strength grade 42.5; the polymer emulsion is pure acrylic emulsion; quartz sand is 50-100 mesh and 70~140 mesh graded quartz ...
Embodiment 2
[0076] A water-based two-component quick-drying polymer cement waterproof mortar, including powder and liquid, wherein the powder is composed of the following components: Portland cement 42%, sulfur-aluminum cement 10%, microcrystalline powder 11% , Quartz sand 35.68%, high-strength anti-cracking fiber 0.65%, water-retaining agent 0.03%, powder defoamer 0.15%, water-reducing agent 0.15%, retarder 0.04%, early-strength agent 0.15%, water-repellent agent 0.15%; The liquid material is composed of the following components: 40% polymer emulsion, 0.2% liquid defoamer, 0.2% preservative, 0.15% pH regulator, and water as the balance.
[0077] The mixing ratio of the above-mentioned powder material and liquid material is 2.8:1 by weight.
[0078] Its preparation method and use method are the same as embodiment 1.
Embodiment 3
[0080] A water-based two-component quick-drying polymer cement waterproof mortar, including powder and liquid, wherein the powder is composed of the following components: Portland cement 44%, sulfoaluminum cement 8%, microcrystalline powder 9% , Quartz sand 37.29%, high-strength anti-cracking fiber 0.95%, water-retaining agent 0.05%, powder defoamer 0.2%, water-reducing agent 0.18%, retarder 0.03%, early-strength agent 0.2%, water-repellent agent 0.1%; The liquid material is composed of the following components: 42% polymer emulsion, 0.25% liquid defoamer, 0.18% preservative, 0.2% pH regulator, and water as the balance.
[0081] The mixing ratio of the above-mentioned powder material and liquid material is 3.2:1 by weight.
[0082] Its preparation method and use method are the same as embodiment 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com