Anti-bacterial anti-mite mulberry silk quilt
A technology for mulberry silk and anti-mite, which is applied in the directions of animal repellents, botanical equipment and methods, biocides, etc., and achieves the effects of simple preparation method, slow release of aroma, and long-term retention of aroma
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0034] The antibacterial and anti-mite mulberry silk quilt can be obtained through the following steps:
[0035] (1) Put the cooked silkworms that have been emptied of feces and urine on the silk spinning net, and the density of cooked silkworms is 800-900 / ㎡. The silk-spinning net is a flat-spinning silk-spinning net with a mesh width of 2-5 mm and a thickness of 1-2 mm.
[0036] (2) After the cooked silkworms have finished silk spinning, the silk is stripped from the spinning net to obtain a smooth fluffy sheet.
[0037] (3) Use a hydrogen peroxide solution with a temperature of 98-100°C and a concentration of 4% by mass for 30-40 minutes to degumming the wool sheet until the sericin content is 2.5-3.5%.
[0038] (4) Clean the degummed cotton sheet with clean water, and then place it in a dehydrator for dehydration.
[0039] (5) After the dehydrated cotton sheet is treated with impurity removal and shaping, it is dried to obtain a dry cotton sheet for later use; the drying ...
Embodiment 2
[0055] The antibacterial and anti-mite mulberry silk quilt can be obtained through the following steps:
[0056] (1) Put the cooked silkworms that have been emptied of feces and urine on the silk spinning net, and the density of cooked silkworms is 800-900 / ㎡. The silk-spinning net is a flat-spinning silk-spinning net with a mesh width of 2-5 mm and a thickness of 1-2 mm.
[0057] (2) After the cooked silkworms have finished silk spinning, the silk is stripped from the spinning net to obtain a smooth fluffy sheet.
[0058] (3) Cook for 30-40 minutes with a hydrogen peroxide solution at a temperature of 98-100°C and a mass percent concentration of 4%, and degumming the wool sheet until the sericin content is 2.5-3.5%; Minutes, add hydrogen peroxide solution weight 1.5-2% ethylene glycol diglycidyl ether.
[0059] (4) Clean the degummed cotton sheet with clean water, and then place it in a dehydrator for dehydration.
[0060] (5) After the dehydrated cotton sheet is treated wi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com