Embodiment 1
[0023] A sand washing process for cotton fabrics, comprising the following steps:
[0024] A. After soaking the fresh shells with hydrochloric acid, wash them with clear water, dry them, and crush them until the particle size is 1-3mm;
[0025] B. Calcining the shell powder at a high temperature of 890°C for 2.5 hours;
[0026] C. further pulverizing the calcined shell powder to a particle size of 200-500 μm to obtain micron shell powder;
[0027] D. Add micron-sized shell powder and cotton fabric into the washing machine, and stir together in warm water at 70°C for 35 minutes;
[0028] E. After taking out the cotton fabric, clean it briefly under acidic conditions, rinse it with clean water, and dry it.
[0029] In the step B, after calcining, the porosity of the shell powder is 12-15%.
[0030] In the step D, the dosage ratio of shell powder to cotton fabric is 2.5:10.
[0031] In the step E, the acidic condition is a slightly acidic condition with a pH of 6.0.
Embodiment 2
[0033] A sand washing process for cotton fabrics, comprising the following steps:
[0034] A. After soaking the fresh shells with hydrochloric acid, wash them with clear water, dry them, and crush them until the particle size is 1-3mm;
[0035] B. Calcining the shell powder at a high temperature of 900°C for 4 hours;
[0036] C. further pulverizing the calcined shell powder to a particle size of 200-500 μm to obtain micron shell powder;
[0037] D. Add micron-sized shell powder and cotton fabric into the washing machine, and stir together in warm water at 60°C for 40 minutes;
[0038] E. After taking out the cotton fabric, clean it briefly under acidic conditions, rinse it with clean water, and dry it.
[0039] In the step B, after calcining, the porosity of the shell powder is 10-12%.
[0040] In the step D, the dosage ratio of shell powder and cotton fabric is 3:10.
[0041] In the step E, the acidic condition is a slightly acidic condition with a pH of 5.5.
Embodiment 3
[0043] A sand washing process for cotton fabrics, comprising the following steps:
[0044] A. After soaking the fresh shells with hydrochloric acid, wash them with clear water, dry them, and crush them until the particle size is 1-3mm;
[0045] B. Calcining the shell powder at a high temperature of 880°C for 2 hours;
[0046] C. further pulverizing the calcined shell powder to a particle size of 200-500 μm to obtain micron shell powder;
[0047] D. Add micron-sized shell powder and cotton fabric into the washing machine, and stir together in warm water at 80°C for 30 minutes;
[0048] E. After taking out the cotton fabric, clean it briefly under acidic conditions, rinse it with clean water, and dry it.
[0049] In the step B, after calcining, the porosity of the shell powder is 16-20%.
[0050] In the step D, the dosage ratio of shell powder and cotton fabric is 2:10.
[0051] In the step E, the acidic condition is a slightly acidic condition with a pH of 6.2.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
porosity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com