Preparation method of novel energy-saving and environment-friendly building material
An energy-saving, environmentally friendly, and building materials technology, applied in the field of building materials, can solve the problems of unsatisfactory heat insulation effect, high additive amount, and lack of crack resistance, etc., and achieve the effects of improving fusion performance, good flame retardancy, and low cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] A preparation method of a novel energy-saving and environment-friendly building material, comprising the following steps:
[0027] 1. At the temperature of the disperser at 120°C, add nano-oxides into the disperser and stir for 14 minutes to preheat, adjust the speed of the disperser to 1000 rpm / min, slowly add the refractory material into the disperser, disperse and stir for 50 minutes, and obtain mixture 1;
[0028] 2. Take silicon dioxide powder and nano-silicon carbide powder by mass ratio, and use dehydrated alcohol as a dispersion medium for the silicon dioxide and silicon carbide powder that has been weighed, and obtain mixture 2 after dispersion;
[0029] 3. Add water-soluble binder hydroxypropyl methylcellulose to mixture 2, and use agate balls as grinding balls to obtain mixture 3 after ball milling;
[0030] 4. Pour the mixture 3 together with the agate balls into the powder tray, dry and sieve at 130°C, take out the agate balls, and grind to obtain the mixtu...
Embodiment 2
[0040] A preparation method of a novel energy-saving and environment-friendly building material, comprising the following steps:
[0041] 1. At the disperser temperature of 120°C, add nano-oxides into the disperser, stir and preheat for 15 minutes, adjust the speed of the disperser to 1000 rpm / min, slowly add the refractory material into the disperser, disperse and stir for 50 minutes, and obtain mixture 1;
[0042] 2. Take silicon dioxide powder and nano-silicon carbide powder by mass ratio, and use dehydrated alcohol as a dispersion medium for the silicon dioxide and silicon carbide powder that has been weighed, and obtain mixture 2 after dispersion;
[0043] 3. Add water-soluble binder hydroxypropyl methylcellulose to mixture 2, and use agate balls as grinding balls to obtain mixture 3 after ball milling;
[0044] 4. Pour the mixture 3 together with the agate balls into the powder tray, dry and sieve at 130°C, take out the agate balls, and grind to obtain the mixture 4;
...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com