Metal anticorrosive material, and preparation method thereof
A metal anti-corrosion and raw material technology, applied in anti-corrosion coatings, epoxy resin coatings, coatings, etc., to achieve the effect of good surface toughness, good thixotropy and strong adhesion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0034] A metal anti-corrosion material, comprising the following raw materials in parts by weight: 75 parts of epoxy resin, 25 parts of mixed solvent, 1.75 parts of toughening agent, 0.35 parts of defoamer, 10 parts of phenalkamine epoxy curing agent, 2.2 parts of anti-aging agent , 0.8 parts of antioxidant, 0.45 parts of lubricant, 0.9 parts of thixotropic agent, 2 parts of pigment and 20 parts of filler;
[0035] The mixed solvent is ethanol, butanone and DBE with a weight ratio of 1:2:7.
[0036] The toughening agent is nano-silica or liquid polysulfide rubber. After curing, the epoxy resin has low elongation and high brittleness. When the bonded part is subjected to external force, cracks are prone to occur and develop rapidly, resulting in cracking of the anti-corrosion coating; nano-dioxide Silicon has strong rigidity, and when the crack expands, it will deflect when encountering nano-silica particles, thereby absorbing energy and achieving the purpose of toughening; liq...
Embodiment 2
[0051] A metal anticorrosion material, comprising the following raw materials in parts by weight: 70 parts of epoxy resin, 20 parts of mixed solvent, 0.5 part of toughening agent, 0.2 part of defoamer, 4 parts of phenalkamine epoxy curing agent, and 1.2 parts of anti-aging agent , 0.1 part of antioxidant, 0.1 part of lubricant, 0.5 part of thixotropic agent, 1 part of pigment and 15 parts of filler;
[0052] The mixed solvent is ethanol, butanone and DBE with a weight ratio of 1:1.8:6.5.
[0053] The toughening agent is nano-silica or liquid polysulfide rubber. After curing, the epoxy resin has low elongation and high brittleness. When the bonded part is subjected to external force, cracks are prone to occur and develop rapidly, resulting in cracking of the anti-corrosion coating; nano-dioxide Silicon has strong rigidity, and when the crack expands, it will deflect when encountering nano-silica particles, thereby absorbing energy and achieving the purpose of toughening; liquid...
Embodiment 3
[0068] A metal anti-corrosion material, comprising the following raw materials in parts by weight: 80 parts of epoxy resin, 30 parts of mixed solvent, 3 parts of toughening agent, 0.5 part of defoamer, 16 parts of phenalkamine epoxy curing agent, 3.2 parts of anti-aging agent , 1.5 parts of antioxidant, 0.8 parts of lubricant, 1.3 parts of thixotropic agent, 3 parts of pigment and 25 parts of filler;
[0069] The mixed solvent is ethanol, butanone and DBE with a weight ratio of 1:2.2:7.5.
[0070] The toughening agent is nano-silica or liquid polysulfide rubber. After curing, the epoxy resin has low elongation and high brittleness. When the bonded part is subjected to external force, cracks are prone to occur and develop rapidly, resulting in cracking of the anti-corrosion coating; nano-dioxide Silicon has strong rigidity, and when the crack expands, it will deflect when encountering nano-silica particles, thereby absorbing energy and achieving the purpose of toughening; liqui...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com