A technology for signal transmission and sheathing material, applied in rubber insulators, organic insulators, etc., can solve the problems of unsatisfactory antibacterial properties of cable sheaths, increased risk of sheath rupture, affecting cable transmission performance, etc., and achieves good processing performance. The effect of low toxicity and long service life
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0030] The raw materials of the sheath are: 800 parts of neoprene CR-121, 200 parts of natural rubber, 50 parts of nano-zinc oxide, 40 parts of magnesium oxide, 13 parts of accelerator TMTD, 12 parts of accelerator DM, 20 parts of anti-aging agent MB, anti-aging 10 parts of agent 4010NA, 350 parts of high wear-resistant carbon black, 20 parts of stearic acid, 40 parts of microcrystalline paraffin, 120 parts of clay, 30 parts of dioctyl ester, 410 parts of nano calcium carbonate, 120 parts of rubber antifungal agent AEM5700-XJ , Anti-yellowing finishing agent TF-621 110 parts.
[0031] The preparation method is as follows: (1) After adding neoprene and natural rubber into the internal mixer according to the formula ratio, then add half of the formula ratio, a compounding agent consisting of magnesium oxide, nano-zinc oxide, accelerator and anti-aging agent, and then add High wear-resistant carbon black and engine oil in the formula ratio, the temperature of the internal mixer i...
Embodiment 2
[0035] The raw materials of the sheath are: 700 parts of neoprene CR-121, 160 parts of natural rubber, 45 parts of nano-zinc oxide, 36 parts of magnesium oxide, 15 parts of accelerator TMTD, 13 parts of accelerator DM, 18 parts of anti-aging agent MB, anti-aging 8 parts of agent 4010NA, 300 parts of high wear-resistant carbon black, 18 parts of stearic acid, 38 parts of microcrystalline paraffin, 118 parts of clay, 29 parts of dioctyl ester, 400 parts of nano calcium carbonate, 125 parts of rubber antifungal agent AEM5700-XJ, Anti-yellowing finishing agent TF-621 100 parts.
[0036] The preparation method is the same as in Example 1.
Embodiment 3
[0038]The raw materials of the sheath are: 650 parts of neoprene CR-121, 130 parts of natural rubber, 40 parts of nano-zinc oxide, 30 parts of magnesium oxide, 20 parts of accelerator TMTD, 16 parts of accelerator DM, 15 parts of anti-aging agent MB, anti-aging 12 parts of agent 4010NA, 280 parts of high wear-resistant carbon black, 20 parts of stearic acid, 35 parts of microcrystalline paraffin, 100 parts of pottery clay, 28 parts of dioctyl ester, 360 parts of nano-calcium carbonate, 120 parts of rubber antifungal agent AEM5700-XJ, Anti-yellowing finishing agent TF-621 110 parts.
[0039] The preparation method is the same as in Example 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com