A technology of simple explosives and explosives, applied in explosives, non-explosive/non-thermal agent components, offensive equipment, etc., can solve the problems of increasing the cost of explosives and safety risks, and improve the charging environment and labor intensity of workers, as well as excellent explosive performance , obvious economic and social benefits
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0039] The raw material parts by weight of the expanded oil ammonium nitrate aqueous phase consist of: 90 parts of ammonium nitrate, 1 part of sodium nitrate, 0.1 part of dispersant stearic acid, and 8 parts of water;
[0040] The raw material weight percent of ammonium nitrate oil phase of puffed oil is: solid composite oil phase 60%, liquid composite oil phase 40%;
[0041] The weight percent of the raw materials of the viscous explosive is: 20% of porous granular ammonium nitrate, 270% of expanded oil ammonium nitrate, 6% of polyacrylamide solution and 4% of light diesel oil.
Embodiment 2
[0043] The raw material parts by weight of the expanded oil ammonium nitrate aqueous phase consist of: 88 parts of ammonium nitrate, 2 parts of sodium nitrate, 0.2 part of dispersant ethyl stearate, and 6 parts of water;
[0044] The raw material weight percent of ammonium nitrate oil phase of puffed oil is: solid composite oil phase 50%, liquid composite oil phase 50%;
[0045] The weight percent of the raw materials of the viscous explosive is: 75% of porous granular ammonium nitrate, 20% of expanded oil ammonium nitrate, 3.5% of polyacrylamide solution and 1.5% of light diesel oil.
Embodiment 3
[0047] The raw material parts by weight of the puffed oil ammonium nitrate aqueous phase consist of: 95 parts of ammonium nitrate, 0.3 part of dispersant stearic acid, and 9 parts of water;
[0048] The raw material weight percent of ammonium nitrate oil phase of puffed oil is: solid composite oil phase 40%, liquid composite oil phase 60%;
[0049] The weight percent of the raw materials of the viscous explosive is: 25% of porous granular ammonium nitrate, 65% of expanded oil ammonium nitrate, 5.5% of polyacrylamide solution and 4.5% of light diesel oil.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com