Preparation method of barite mineral collecting agent
A collector and barite technology, applied in the direction of solid separation, flotation, etc., to achieve the effect of less reagent consumption, good concentrate grade and good recovery rate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] An example of the preparation method of barite mineral collector of the present invention, comprises the following steps:
[0017] Two or three of peanuts, rapeseed, pine coriander and pine bark are used as raw materials, dried, crushed, passed through a 80-mesh sieve, and taken according to the mass ratio: powder: diethylamine: water = 1:1:3 , heated to 150°C, fed with nitrogen and stirred for 3.5 hours, cooled to below 55°C, filtered, and the filtrate was centrifuged with a centrifugal sedimentation machine, and the supernatant was subjected to vacuum distillation to obtain a dark yellow concentrated solution, which was placed in a 75°C water bath Heat in medium temperature, evaporate the solvent to dryness, and dry the obtained viscous liquid in a vacuum drying oven at a temperature of 50°C to obtain a yellow-brown viscous solid. After complete drying, a yellow powder is obtained, which is the collector of barite minerals.
Embodiment 2
[0019] Another example of the preparation method of the barite mineral collector of the present invention comprises the following steps:
[0020] Two or three of peanuts, rapeseed, pine coriander and pine bark are used as raw materials, dried, crushed, passed through a 80-mesh sieve, and taken according to the mass ratio: powder: diethylamine: water = 3:4:10 , heated to 160°C, fed with nitrogen and stirred for 4 hours, cooled to below 55°C, filtered, and the filtrate was centrifuged with a centrifugal sedimentation machine, and the supernatant was subjected to vacuum distillation to obtain a dark yellow concentrated solution, which was placed in a water bath at 80°C Heating, evaporating the solvent to dryness, and drying the obtained viscous liquid in a vacuum drying oven at a temperature of 50°C to obtain a yellowish-brown viscous solid, and after complete drying, a yellow powder is obtained, which is the collector of barite minerals.
Embodiment 3
[0022] This embodiment is an application example of the barite mineral collector in barite mineral flotation.
[0023] 1. Mineral raw materials:
[0024] The content of barite in the raw ore is 45.67%, silicon 7.23%, and calcium carbonate 5.61%. Silicon mainly exists in the form of silica and a small amount of aluminum-silicon minerals, and calcium carbonate mainly exists in the form of calcite and a small amount of limestone.
[0025] 2. Chemical system and operating conditions: use sodium carbonate to adjust the pH of the pulp to 10.5-11, conduct tests according to water glass 2500g / t, collector dosage 800g / t, No. 2 oil 60g / t dosage, the results show that the above process is adopted And chemical conditions can effectively recover barite minerals by flotation. Under the condition that the barite content of the ore is 45.67%, after one roughing, two sweeping and three selections, the barite grade of the flotation concentrate reaches 95.21% %, the recovery rate reached 81.07%...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com