Biological treatment method for wood fiber hydrolysate
A lignocellulosic and biological treatment technology, applied in the field of biomass refining, can solve the problems of poor selectivity, high loss rate of oligosaccharides, low lignin removal efficiency, etc., to reduce removal rate, reduce loss, improve membrane flux and The effect of production efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0039] A kind of lignocellulosic hydrolyzate biological treatment method, the steps are as follows:
[0040] (1) The hydrolyzed liquid after self-hydrolysis of poplar wood, the content of oligosaccharides is 7.2g / L, the content of lignin is 4.5g / L, and the content of colloidal lignin is 1.4g / L. The hydrolyzate is treated with acid pectinase, and the treatment conditions are: the enzyme dosage is 150g / ton hydrolyzate, the temperature is 40°C, the time is 8h, and the pH is 3.5.
[0041] (2) The hydrolyzate after pectinase treatment is treated with cationic polymer polyallyldimethylammonium chloride, the amount of cationic polymer is 100g / ton of hydrolyzate, the treatment temperature is room temperature, pH3.5, and the time is 5 minutes. After the cationic polymer was treated, it was left to stand for 8 hours, and the precipitate was removed by decantation to obtain the purified hydrolyzate of the upper layer.
[0042] In this example, after pectinase treatment and cationic poly...
Embodiment 2
[0045] A kind of lignocellulosic hydrolyzate biological treatment method, the steps are as follows:
[0046] (1) The hydrolyzed solution after self-hydrolysis of wheat straw has an oligosaccharide content of 4.6 g / L, a lignin content of 3.1 g / L, and a colloidal lignin content of 0.8 g / L. The hydrolyzate is first treated with neutral pectinase, and the treatment conditions are: enzyme dosage 180g / ton of hydrolyzate, temperature 45°C, time 12h, pH 7.0.
[0047] (2) After pectinase treatment, cationic polymer polyethylenimine was used to treat the hydrolyzate at an amount of 85 g / ton, at room temperature, pH 7.0, and for 10 minutes. After the cationic polymer was treated, it was left to stand for 4 hours, and the precipitate was removed by decantation to obtain the purified hydrolyzate of the upper layer. After pectinase-cationic polymer treatment, the removal rate of lignin was 45%, among which the removal rate of colloidal lignin was 90%, and the loss rate of oligosaccharide w...
Embodiment 3
[0050] A kind of lignocellulosic hydrolyzate biological treatment method, the steps are as follows:
[0051] (1) The hydrolyzed solution after self-hydrolysis of spruce, the content of oligosaccharides is 6.8g / L, the content of lignin is 3.9g / L, and the content of colloidal lignin is 1.6g / L. The hydrolyzate is first treated with acid pectinase, and the treatment conditions are: the enzyme dosage is 200g / ton hydrolyzate, the temperature is 50°C, the time is 16h, and the pH is 4.0.
[0052] (2) After pectinase treatment, polyaluminum chloride is used for treatment, the dosage is 200 g / ton of hydrolyzate, the treatment temperature is room temperature, pH 4.0, and the treatment time is 15 minutes. After cationic polymer treatment, centrifuge for 15 minutes to remove the precipitate and obtain the purified hydrolyzate of the upper layer. After pectinase-cation polymer treatment, the removal rate of lignin was 47%, among which the removal rate of colloidal lignin was 91%, and the l...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com