A process and technology of Jun porcelain, applied in the field of Jun porcelain firing technology, can solve the problems of low qualified rate of finished products, complicated production process, waste of raw materials, etc., and achieve the effect of high qualified rate of finished products, reasonable process and simplified labor.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0031] A Jun porcelain firing process, which includes biscuit firing, glazing and glaze firing, and the biscuit firing includes the following steps:
[0032] (1) Billet inspection: inspect the fine billet entering the kiln according to the fine billet standard, and only those who pass the inspection can enter the kiln;
[0033] (2) Kiln loading: the qualified fine blanks are classified according to different varieties and loaded on the supported kiln car shed;
[0034] (3) Entering the kiln: slowly and uniformly push the loaded kiln car into the kiln and close the kiln door;
[0035] (4) Kiln firing: gradually increase the temperature in the kiln from room temperature to 900°C within 4 hours, and then stop the fire;
[0036] (5) Cooling: Cool the temperature in the kiln to 100°C naturally and then open the kiln door to avoid the rapid cooling of the temperature and cause the green body to crack. At this time, pull out the kiln car and take the fired green body;
[0037] Desc...
Embodiment 2
[0054] A Jun porcelain firing process, which includes biscuit firing, glazing and glaze firing, and the biscuit firing includes the following steps:
[0055] (1) Billet inspection: inspect the fine billet entering the kiln according to the fine billet standard, and only those who pass the inspection can enter the kiln;
[0056] (2) Kiln loading: the qualified fine blanks are classified according to different varieties and loaded on the supported kiln car shed;
[0057] (3) Entering the kiln: slowly and uniformly push the loaded kiln car into the kiln and close the kiln door;
[0058] (4) Kiln firing: gradually increase the temperature in the kiln from room temperature to 900°C within 4 hours, and then stop the fire;
[0059] (5) Cooling: Cool the temperature in the kiln to 100°C naturally and then open the kiln door to avoid the rapid cooling of the temperature and cause the green body to crack. At this time, pull out the kiln car and take the fired green body;
[0060] Desc...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com