A wood coating, water-based technology, applied in fireproof coatings, polyurea/polyurethane coatings, coatings, etc., can solve the problems of reduced cold and heat resistance, complicated preparation process, high input cost, etc., to reduce surface tension and adhesion Good, good film-forming effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0047] A preparation method of a water-based wood coating with zero VOC volatilization comprises the following steps:
[0048] Step 1: Stir 63.42 parts by weight of pure water and 0.02 parts of preservative at a speed of 250-320 rpm, then slowly add 5 parts of starch, and heat up while stirring, so that the temperature reaches 90°C , continue to stir for 4-6 minutes, cool to room temperature, then add 1.5 parts of emulsifier and stir for 5 minutes, then add 30 parts of castor oil and stir for 15 minutes at a speed of 2000 rpm, then reduce the speed to 500 rpm and add 0.01 part of water-based defoamer and 0.05 part of water-based catalyst, stirred for 10-20 minutes, filtered to obtain component A.
[0049] Step 2: Prepare component A, component B and purified water in parts by weight of 1:0.4:0.5 to obtain a water-based wood coating with zero VOC volatilization.
Embodiment 2
[0051] A preparation method of a water-based wood coating with zero VOC volatilization comprises the following steps:
[0052] Step 1: Stir 64.52 parts by weight of pure water and 0.02 parts of preservative at a speed of 250-320 rpm, then slowly add 6 parts of starch, and heat up while stirring, so that the temperature reaches 90°C , continue to stir for 4-6 minutes, cool to room temperature, add 1.4 parts of emulsifier and stir for 5 minutes, then add 28 parts of castor oil and stir for 15 minutes at a speed of 2000 rpm, then reduce the speed to 500 rpm and add 0.01 part of water-based defoamer and 0.05 part of water-based catalyst, stirred for 10-20 minutes, filtered to obtain component A.
[0053] Step 2: Prepare component A, component B and purified water in parts by weight of 1:0.4:0.5 to obtain a water-based wood coating with zero VOC volatilization.
Embodiment 3
[0055] A preparation method of a water-based wood coating with zero VOC volatilization comprises the following steps:
[0056] Step 1: Stir 65.62 parts by weight of pure water and 0.02 parts of preservative at a speed of 250-320 rpm, then slowly add 7 parts of starch, and heat up while stirring, so that the temperature reaches 90°C , continue to stir for 4-6 minutes, cool to room temperature, add 1.3 parts of emulsifier and stir for 5 minutes, then add 26 parts of castor oil and stir for 15 minutes at a speed of 2000 rpm, then reduce the speed to 500 rpm and add 0.01 part of water-based defoamer and 0.05 part of water-based catalyst, stirred for 10-20 minutes, filtered to obtain component A.
[0057] Step 2: Prepare component A, component B and purified water in parts by weight of 1:0.4:0.5 to obtain a water-based wood coating with zero VOC volatilization.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com