[0024] An environment-friendly high-life antifouling real stone paint, which is made of the following components in parts by weight: pure acrylic emulsion 35-38, ethyl silicate 0.1-0.2, tapioca starch 0.4-0.6, modified gum arabic 1.0-1.2, Castor oil 0.8-1.0, active silica fume powder 0.6-0.8, dispersant 0.3-0.4, sodium dodecylsulfonate 0.7-0.9, polyurethane thickener 0.4-0.6, film-forming aid 1.2-1.5, hollow glass micro Pearl 0.6-1.0, defoamer 0.1-0.2, lotus leaf pulp water 24-30, natural colored sand 65-68, modified wood fiber 0.6-0.8;
[0025] The preparation method of the modified wood fiber is as follows: add deionized water of 10 times its mass to the wood fiber, stir at a speed of 120r / min and heat up to 78°C, add 0.2% of the wood fiber mass ascorbic acid, Stir at a speed of 10 min / min, continue heating to 86°C, then add sodium hydroxide with a mass of 1.2% of the wood fiber mass, stir at a speed of 120r / min for 20 min, keep warm at 80-82°C, and add 1.8% of the mass of w...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com