Preparation method of bobbin paper
A bobbin paper and waste paper technology, applied in the directions of non-woody plant/crop pulp, secondary cellulose fibers, etc., can solve the problems of breaking industry rules, poor bobbin paper quality, poor paper quality, etc., to reduce damage , sufficient raw materials, the effect of reducing damage and pollution
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A method for preparing bobbin paper comprises the following weight ratios: 15 parts of bagasse pulp, 8 parts of fluff fiber, and 28 parts of banana stem pulp, and then put 15 parts of bagasse pulp, 8 parts of fluff fiber, and 28 parts of banana stem pulp into Fully stir in the mixer, and raise the temperature to 60°C to activate the internal cellulose, and then go through the steps of screen separation, filter cleaning, fiber grinding, dehydration separator dehydration, and then add the following weight ratio: 17 parts of American waste paper , 35 parts of domestic waste paper, and diluted with water, the ratio of slurry to water is 3:5, then add papermaking additives and fillers, and carry out heating and stirring, the temperature is raised to 70 ° C, and then through papermaking, drying and shearing into the desired Needed bobbin paper.
[0022] The tensile properties of 15 parts of bagasse pulp, 8 parts of fluff fiber and 28 parts of banana stem pulp after stirring a...
Embodiment 2
[0027] A method for preparing bobbin paper comprises the following weight ratios: 18 parts of bagasse pulp, 11 parts of fluff fiber, and 31 parts of banana stem pulp, and then put 18 parts of bagasse pulp, 11 parts of fluff fiber, and 31 parts of banana stem pulp Stir fully in the mixer, and increase the temperature to 60°C to activate the internal cellulose, and then go through the steps of screen separation, filter cleaning, fiber grinding, and dehydration with a dehydrator, and then add the following weight ratio: US waste paper 24 39 parts, 39 parts of domestic waste paper, and diluted with water, the ratio of slurry to water is 4:7, then add papermaking additives and fillers, and carry out heating and stirring, the temperature is raised to 70 ° C, and then after papermaking, drying and shearing into The required bobbin paper.
[0028] The 18 parts of bagasse pulp, 11 parts of fluff fiber and 31 parts of banana stem pulp after being stirred have a tensile property ≥ 8kn / m,...
Embodiment 3
[0033] A method for preparing bobbin paper comprises the following weight ratios: 21 parts of bagasse pulp, 12 parts of fluff fiber, and 32 parts of banana stem pulp, and then put 21 parts of bagasse pulp, 12 parts of fluff fiber, and 32 parts of banana stem pulp into Fully stir in the mixer, and increase the temperature to 60°C to activate the internal cellulose, and then go through the steps of screen separation, filter cleaning, fiber grinding, and dehydration with a dehydrator, and then add the following weight ratio: 25 parts of American waste paper , 46 parts of domestic waste paper, and diluted with water, the ratio of slurry to water is 6:9, then add papermaking additives and fillers, and carry out heating and stirring, the temperature is raised to 70 ° C, and then through papermaking, drying and shearing into the Needed bobbin paper.
[0034] The tensile properties of 21 parts of bagasse pulp, 12 parts of fluff fiber and 32 parts of banana stem pulp after stirring are...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com