PU xanthochromia-resisting tripolymer curing agent formula and producing method
A production method and trimer technology, applied in the direction of polyurea/polyurethane adhesives, adhesives, adhesive types, etc., can solve the problems of complicated production process methods, high production costs, large equipment investment, etc. Gloss, increase compatibility, increase the effect of yellowing resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0010] Example 1, Step 1: Add ethyl acetate, 1.5% antioxidant, 475% BASF toluene diisocyanate, and 10% dodecyl alcohol to the reactor in sequence, and then heat up to 70°C to 75°C. ℃ and heat preservation; Step 2: Add ethyl acetate with a weight ratio of 200 into the reactor, and after the temperature in the reactor drops to 65°C, add an initiator with a mass ratio of 0.2 and a catalyst with a mass ratio of 1.6 and dilute with ethyl acetate Stir the mixed solvent evenly, keep it warm for 1.5-2 hours and detect the percentage value of NCO group content. Step 3: When monitoring the content of NCO groups to be 8.5%-8.7%, immediately add terminator phosphoric acid with a weight ratio of 0.6 diluted with butyl acetate and stir the mixed solvent in the reactor when adding, and the stirring time is long In 0.5 hours; Step 4: Add butyl acetate with a mass ratio of 100 and an ultraviolet absorber UV of 0.3, and stir evenly. Add butyl acetate, 50% base material, and 35% HDI trimer in s...
Embodiment 2
[0013] Embodiment two, PU anti-yellowing trimer curing agent formula and production method, comprise the following steps: Step 1: in reaction kettle, add the ethyl acetate of 209.6, the antioxidant of 1.5, the BASF of 475 successively in weight ratio respectively Mix toluene diisocyanate and 10% dodecyl alcohol, heat up to 70°C to 75°C and keep warm; Step 2: Add ethyl acetate with a weight ratio of 200 into the reactor, and wait until the temperature in the reactor drops to 65°C Add an initiator with a mass ratio of 0.2 and a catalyst with a mass ratio of 1.6 and mix well with the mixed solvent diluted with ethyl acetate, keep it warm for 1.5-2 hours and detect the percentage value of the NCO group content, and the holding temperature value is 65°C to 70°C , during the heat preservation stage, adding ethyl acetate with a weight ratio of 2 and a catalyst with a weight ratio of 0.2 is placed in the reactor and stirred evenly to continue the heat preservation; Step 3: When the con...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com