[0019] Embodiment 1: the preparation of composition
[0020] Raw material weight ratio:
[0021] Heavy calcium carbonate, 30 parts; Light calcium carbonate, 10 parts; Bentonite, 20 parts; Wollastonite, 10 parts; Borax, 15 parts; Yuanming powder, 10 parts; Zeolite powder, 10 parts; Barite powder, 15 parts; diatomaceous earth powder, 40 parts; the mixture of barium sulfate powder and chitosan, 5 parts; the weight ratio of described barium sulfate powder and chitosan is 4:1.
[0022] Preparation:
[0023] Step S1, grinding the dried heavy calcium carbonate, light calcium carbonate, wollastonite, sodium sulfate and barite powder together, with a fineness of 0.07-0.08mm;
[0024] Step S2, grinding the dried bentonite, borax, zeolite powder and diatomaceous earth powder together to a fineness of 0.05-0.07mm;
[0025] Step S3, grinding the dried barium sulfate powder and chitosan together to a fineness of 0.04-0.06mm;
[0026] In step S4, the fine powders ground in steps S1, S2, ...
Embodiment 2
[0028] Embodiment 2: the preparation of composition
[0029] Raw material weight ratio:
[0030] Heavy calcium carbonate, 25 parts; Light calcium carbonate, 5 parts; Bentonite, 15 parts; Wollastonite, 5 parts; Borax, 10 parts; Yuanming powder, 5 parts; Zeolite powder, 5 parts; Barite powder, 10 parts; diatomite powder, 35 parts; the mixture of barium sulfate powder and chitosan, 4 parts; the weight ratio of described barium sulfate powder and chitosan is 3:1.
[0031] Preparation:
[0032] Step S1, grinding the dried heavy calcium carbonate, light calcium carbonate, wollastonite, sodium sulfate and barite powder together, with a fineness of 0.07-0.08mm;
[0033] Step S2, grinding the dried bentonite, borax, zeolite powder and diatomaceous earth powder together to a fineness of 0.05-0.07mm;
[0034] Step S3, grinding the dried barium sulfate powder and chitosan together to a fineness of 0.04-0.06mm;
[0035] In step S4, the fine powders ground in steps S1, S2, and S3 are ev...
Embodiment 3
[0037] Embodiment 3: the preparation of composition
[0038] Raw material weight ratio:
[0039] Heavy calcium carbonate, 35 parts; Light calcium carbonate, 15 parts; Bentonite, 25 parts; Wollastonite, 15 parts; Borax, 20 parts; Yuanming powder, 15 parts; Zeolite powder, 15 parts; Barite powder, 20 parts; diatomaceous earth powder, 45 parts; the mixture of barium sulfate powder and chitosan, 6 parts; the weight ratio of described barium sulfate powder and chitosan is 5:1.
[0040] Preparation:
[0041] Step S1, grinding the dried heavy calcium carbonate, light calcium carbonate, wollastonite, sodium sulfate and barite powder together, with a fineness of 0.07-0.08mm;
[0042] Step S2, grinding the dried bentonite, borax, zeolite powder and diatomaceous earth powder together to a fineness of 0.05-0.07mm;
[0043] Step S3, grinding the dried barium sulfate powder and chitosan together to a fineness of 0.04-0.06mm;
[0044] In step S4, the fine powders ground in steps S1, S2, ...
PUM
Property | Measurement | Unit |
---|---|---|
Fineness | aaaaa | aaaaa |
Fineness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com