A cable sheathing and aging-resistant technology, which is applied in the field of high-temperature and aging-resistant cable sheathing materials and its preparation, can solve problems such as aging, tearing, and safety hazards, and achieve the effect of good high temperature resistance and prolonging service life.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] (1) Add 60 parts of nitrile rubber, 12 parts of diethylene glycol monoethyl ether acetate, 2 parts of magnesium stearate, 10 parts of 2,2,2-trichloroacetamide benzyl ester and 4 parts of acetazolamide to the reaction In the kettle, raise the temperature to 40°C, and mix to a homogeneous state after high-speed stirring;
[0017] (2) Stir 25 parts of methyl vinyl silicone rubber, 3 parts of zinc oxide, 1 part of ferrocene hydrochloride, 11 parts of ethopabate, and 10 parts of carboxybenfen in the reactor for 10 minutes, then Raise the temperature to 50°C and continue the reaction for 20 minutes;
[0018] (3) Add the product obtained in step (2) and the product obtained in step (1) to a high-speed mixer for mixing, then add 3 parts of zirconia magnesium aluminum oxide, 4 parts of zirconocene dichloride, and 12 parts of hydrogenated palm kernel oil The cable sheath material can be obtained after extrusion and granulation in a twin-screw extruder; wherein the screw length-t...
Embodiment 2
[0020] (1) Add 80 parts of nitrile rubber, 18 parts of diethylene glycol monoethyl ether acetate, 7 parts of magnesium stearate, 16 parts of 2,2,2-trichloroacetamide benzyl ester and 10 parts of acetazolamide to the reaction In the kettle, raise the temperature to 60°C, and mix to a homogeneous state after high-speed stirring;
[0021] (2) Stir 35 parts of methyl vinyl silicone rubber, 8 parts of zinc oxide, 4 parts of ferrocene hydrochloride, 18 parts of ethopabate and 15 parts of carboxybenfen in the reactor for 20 minutes, then Raise the temperature to 70°C and continue the reaction for 30 minutes;
[0022] (3) Add the product obtained in step (2) and the product obtained in step (1) to a high-speed mixer for mixing, then add 7 parts of zirconia magnesium aluminum oxide, 7 parts of zirconocene dichloride, and 18 parts of hydrogenated palm kernel oil The cable sheath material can be obtained after extrusion and granulation in a twin-screw extruder; wherein the screw length-...
Embodiment 3
[0024] (1) Add 65 parts of nitrile rubber, 14 parts of diethylene glycol monoethyl ether acetate, 3 parts of magnesium stearate, 12 parts of 2,2,2-trichloroacetamide benzyl ester and 6 parts of acetazolamide to the reaction In the kettle, raise the temperature to 40°C, and mix to a homogeneous state after high-speed stirring;
[0025] (2) Stir 25 parts of methyl vinyl silicone rubber, 4 parts of zinc oxide, 2 parts of ferrocene hydrochloride, 13 parts of ethopabate, and 12 parts of carboxybenfen in the reactor for 10 minutes, then Raise the temperature to 50°C and continue the reaction for 20 minutes;
[0026] (3) Add the product obtained in step (2) and the product obtained in step (1) to a high-speed mixer and mix, then add 4 parts of zirconia magnesium aluminum, 5 parts of zirconocene dichloride, and 13 parts of hydrogenated palm kernel oil The cable sheath material can be obtained after extrusion and granulation in a twin-screw extruder; wherein the screw length-to-diamet...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com