Method for detection of arsenic in underground water
A detection method and groundwater technology, applied in material excitation analysis, Raman scattering, etc., can solve the problems of lack of independent innovation technology in arsenic speciation analysis, weak research and development in the field of field monitoring, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0017] Embodiment 1 gets 0.1 gram of Fe 3 o 4 After washing the nanoparticles several times with absolute ethanol, transfer them into a 100mL three-necked round bottom flask, add 50mL of absolute ethanol to disperse the particles, then add 1mL APTMS and stir evenly for 3.5h. The obtained product was washed with absolute ethanol before use. Take the Fe modified by APTMS 3 o 4 Add 18 mL of silver nitrate solution with a concentration of 0.02 g / mL and 20 μL of potassium hydroxide solution with a concentration of 0.032 g / mL in a 100 mL three-necked round-bottomed flask, and stir evenly. 800 μL of aqueous ammonia, 1 mL of silver nitrate solution with a concentration of 0.06 g / mL, and 40 μL of aqueous ammonia with a concentration of 5% was added dropwise. After stirring for 5 minutes, add 3 mL of anhydrous methanol, 10 μL of sodium polyphosphate solution with a concentration of 0.1 g / mL, and 40 μL of a solution of disodium hydrogen phosphate with a concentration of 0.05 g / mL. F...
Embodiment 2
[0018] Embodiment 2 gets 0.1 gram of Fe 3 o 4 Nanoparticles were washed several times with absolute ethanol, then transferred into a 100mL three-necked round-bottomed flask, 50mL of absolute ethanol was added to disperse the particles, and then 2mL APTMS was added and stirred evenly for 3.5h. The obtained product was washed with absolute ethanol before use. Take the Fe modified by APTMS 3 o 4 Nanoparticles were placed in a 100mL three-necked round bottom flask, and 36mL of silver nitrate solution with a concentration of 0.02g / mL and 20μL of potassium hydroxide solution with a concentration of 0.032g / mL were added and stirred evenly, and the mixed solution was added dropwise with a concentration of 25 % ammonia water 1mL, the concentration is 0.06g / mL silver nitrate solution 1.5mL, and then the concentration is 6% ammonia water 150μL. After stirring for 5 minutes, add 6 mL of anhydrous methanol, 20 μL of sodium polyphosphate solution with a concentration of 0.1 g / mL, and 80...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com