Aqueous high-gloss gloss oil used for artificial leather and preparation method thereof
A technology of synthetic leather and high-gloss light, which is applied in the direction of improved hand-feeling fibers, etc., to achieve the effect of safe and reliable processing, unique hand feel and low viscosity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0033] The water-based high-gloss varnish for synthetic leather is composed of the following components: 150 parts by weight of 1000 molecular weight BG-AA diol (polybutylene adipate), DMPA (2,2-dimethylol propionic acid ) 10 parts by weight, BDO (1,4-butanediol) 5 parts by weight, reactive simethicone 1 part by weight, IPDI (isophorone diisocyanate) 100 parts by weight, acetone 20 parts by weight, triethylamine 5 parts by weight, 10 parts by weight of ethylenediamine, 500 parts by weight of water, 1 part by weight of water-based defoamer, 5 parts by weight of leveling agent and 15 parts by weight of thickener.
[0034] The preparation method of the above water-based high-gloss varnish for synthetic leather is:
[0035] (1) 150 parts by weight of 1000 molecular weight BG-AA dihydric alcohol, 10 parts by weight of DMPA, 5 parts by weight of BDO, and reactive simethicone oil of 1 part by weight are mixed, heated and melted;
[0036] (2) Add 100 parts by weight of IPDI to the mi...
Embodiment 2
[0041]The water-based high-gloss varnish for synthetic leather is composed of the following components: 160 parts by weight of 1000 molecular weight BG-AA diol, 14 parts by weight of DMPA, 7 parts by weight of BDO, 1.5 parts by weight of reactive simethicone oil, 120 parts by weight of IPDI, 30 parts by weight of acetone, 8 parts by weight of triethylamine, 14 parts by weight of ethylenediamine, 550 parts by weight of water, 1.5 parts by weight of water-based defoamer, 7 parts by weight of leveling agent and 18 parts by weight of thickener.
[0042] The preparation method of the above water-based high-gloss varnish for synthetic leather is:
[0043] (1) 160 parts by weight of 1000 molecular weight BG-AA dihydric alcohol, 14 parts by weight of DMPA, 7 parts by weight of BDO, and reactive simethicone oil of 1.5 parts by weight are mixed, heated and melted;
[0044] (2) Add 120 parts by weight of IPDI to the mixture obtained in step (1) and react at 70° C. for 5 hours;
[0045] ...
Embodiment 3
[0049] The water-based high gloss varnish for synthetic leather is composed of the following components: 180 parts by weight of 1000 molecular weight BG-AA diol, 18 parts by weight of DMPA, 12 parts by weight of BDO, 2 parts by weight of reactive simethicone oil, 140 parts by weight of IPDI, 35 parts by weight of acetone, 12 parts by weight of triethylamine, 18 parts by weight of ethylenediamine, 600 parts by weight of water, 2 parts by weight of water-based defoamer, 12 parts by weight of leveling agent and 22 parts by weight of thickener.
[0050] The preparation method of the above water-based high-gloss varnish for synthetic leather is:
[0051] (1) 180 parts by weight of 1000 molecular weight BG-AA dihydric alcohol, 18 parts by weight of DMPA, 12 parts by weight of BDO, and reactive simethicone oil of 2 parts by weight are mixed, heated and melted;
[0052] (2) Add 140 parts by weight of IPDI to the mixture obtained in step (1) and react at 70° C. for 5 hours;
[0053] (...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com