Preparation method for fabrics finishing liquid
A technology for fabric finishing and finishing liquid, applied in fiber treatment, textile and papermaking, improved hand-feeling fibers, etc., can solve the problem that the finishing liquid has a single function, the fabric texture is not soft enough, and cannot meet the antistatic, flame-retardant, anti-static and anti-static requirements of the fabric. Moth, mildew, antibacterial and washable, etc., to achieve excellent antistatic, soft feel, good hydrophilic effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] A preparation method of a fabric finishing solution, comprising the steps of:
[0018] 1) Put 1-2 parts by weight of polyoxyethylene oleate, 1.3 parts by weight of sodium polyacrylate, 1.6 parts by weight of diethylenetriamine, and 2.6 parts by weight of acetic acid into 18 parts by weight of deionized water in sequence, and stir evenly;
[0019] 2) Add 1.3 parts by weight of comfrey extract, 1.1 parts by weight of 3-iodo-2-propynylbutyl carbamate, 0.8 parts by weight of antimony trioxide, and 0.9 parts by weight of isocyanuric acid, and continue stirring , until fully mixed evenly, to prepare a finishing solution.
Embodiment 2
[0021] The preparation method of fabric finishing liquid, comprises the steps:
[0022] 1) Put 1 part by weight of polyoxyethylene oleate, 1.3 parts by weight of sodium polyacrylate, 1.6 parts by weight of diethylenetriamine, and 2.6 parts by weight of acetic acid into 18 parts by weight of deionized water in sequence, and stir evenly;
[0023] 2) Add 1.3 parts by weight of comfrey extract, 1.1 parts by weight of 3-iodo-2-propynylbutyl carbamate, 0.8 parts by weight of antimony trioxide, and 0.9 parts by weight of isocyanuric acid, and continue stirring , until fully mixed evenly, to prepare a finishing solution.
Embodiment 3
[0025] The preparation method of fabric finishing liquid, comprises the steps:
[0026] 1) Put 2 parts by weight of polyoxyethylene oleate, 1.3 parts by weight of sodium polyacrylate, 1.6 parts by weight of diethylenetriamine, and 2.6 parts by weight of acetic acid into 18 parts by weight of deionized water in sequence, and stir evenly;
[0027] 2) Add 1.3 parts by weight of comfrey extract, 1.1 parts by weight of 3-iodo-2-propynylbutyl carbamate, 0.8 parts by weight of antimony trioxide, and 0.9 parts by weight of isocyanuric acid, and continue stirring , until fully mixed evenly, to prepare a finishing solution.
PUM

Abstract
Description
Claims
Application Information

- Generate Ideas
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com