[0020] A method for finishing anti-wrinkle fabrics, comprising the steps of:
[0021] 1) Add 1 to 2 parts by mass of ammonium dihydrogen phosphate, 2.2 parts by mass of potassium dodecyl phosphate, 1.4 parts by mass of polyhexamethylene guanidine phosphate, and 2.4 parts by mass of superfine pearl powder in 22 parts by mass of deionized water. , stir evenly;
[0022] 2) Slowly add 0.8 parts by mass of glycerol monostearate, 2.1 parts by mass of gum arabic powder, 2.7 parts by mass of tetrahydroxyethylphosphine chloride, and 0.9 parts by mass of polypropylene glycol at the same time, and continue to stir until fully mixed and uniform. Finishing agent;
[0023] 3) Pad the fabric in the dipping solution containing the finishing agent, and dry it at a constant temperature.
Embodiment 2
[0025] The finishing method of anti-wrinkle fabric comprises the following steps:
[0026] 1) Put 1 mass part of ammonium dihydrogen phosphate, 2.2 mass parts of potassium dodecyl phosphate, 1.4 mass parts of polyhexamethylene guanidine phosphate, and 2.4 mass parts of superfine pearl powder into 22 mass parts of deionized water, mix, and stir Uniform;
[0027] 2) Slowly add 0.8 parts by mass of glycerol monostearate, 2.1 parts by mass of gum arabic powder, 2.7 parts by mass of tetrahydroxyethylphosphine chloride, and 0.9 parts by mass of polypropylene glycol at the same time, and continue to stir until fully mixed and uniform. Finishing agent;
[0028] 3) Pad the fabric in the dipping solution containing the finishing agent, and dry it at a constant temperature.
Embodiment 3
[0030] The finishing method of anti-wrinkle fabric comprises the following steps:
[0031] 1) Add 2 parts by mass of ammonium dihydrogen phosphate, 2.2 parts by mass of potassium dodecyl phosphate, 1.4 parts by mass of polyhexamethylene guanidine phosphate, and 2.4 parts by mass of superfine pearl powder into 22 parts by mass of deionized water, and stir Uniform;
[0032] 2) Slowly add 0.8 parts by mass of glycerol monostearate, 2.1 parts by mass of gum arabic powder, 2.7 parts by mass of tetrahydroxyethylphosphine chloride, and 0.9 parts by mass of polypropylene glycol at the same time, and continue to stir until fully mixed and uniform. Finishing agent;
[0033] 3) Pad the fabric in the dipping solution containing the finishing agent, and dry it at a constant temperature.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com