Wall paint for purifying formaldehyde
A technology for wall paint and formaldehyde, applied in the direction of coating, etc., can solve the problems that are not many and cannot meet the requirements of purifying formaldehyde
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0018] A purifying formaldehyde wall paint, the preparation method of which comprises a pulping part, a dispersing part and a paint mixing part, wherein the preparation part is made of the following components by weight ratio: deionized water 12%, cellulose 0.16%, wetting agent 0.6%, defoamer 0.25%, antifreeze 1.8%, dispersant 0.9%, multifunctional additive 0.12%.
[0019] The preparation method of the pulping part is as follows: first, start the mixing tank, and set its rotating speed to 400 revolutions per minute, pour the deionized water with the above weight ratio into the mixing tank, and after stirring for 3 minutes, reduce the rotating speed of the mixing tank to 400 rpm. Set at 300 revolutions per minute, the indoor temperature of the pulping part is 26°C, put in the cellulose in the above weight ratio, stir for 4 minutes, put in the wetting agent in the above weight ratio, stir for 2 minutes, put in the above weight ratio of Antifoaming agent, after stirring for 3 min...
Embodiment 2
[0026] A purifying formaldehyde wall paint, its preparation method comprises a pulping part, a dispersing part and a paint mixing part, and the said preparation part is made of the following components by weight ratio: deionized water 16%, cellulose 0.18%, wetting agent 0.7%, defoamer 0.28%, antifreeze 2%, dispersant 0.8%, multifunctional additive 0.15%.
[0027] The preparation method of the pulping part is as follows: first, start the mixing tank, and set its rotating speed to 400 revolutions per minute, pour the deionized water with the above weight ratio into the mixing tank, and after stirring for 3 minutes, reduce the rotating speed of the mixing tank to 400 rpm. Set at 300 revolutions per minute, the indoor temperature of the pulping part is 28°C, put in the cellulose in the above weight ratio, stir for 4 minutes, put in the wetting agent in the above weight ratio, stir for 2 minutes, put in the above weight ratio After stirring for 3 minutes, drop into the antifreeze a...
Embodiment 3
[0034] A purifying formaldehyde wall paint, the preparation method of which comprises a pulping part, a dispersing part and a paint mixing part, wherein the preparation part is made of the following components by weight ratio: deionized water 18%, cellulose 0.19%, wetting agent 0.55%, defoamer 0.23%, antifreeze 2.4%, dispersant 1%, multifunctional additive 0.18%.
[0035] The preparation method of the pulping part is as follows: first, start the mixing tank, and set its rotating speed to 400 revolutions per minute, pour the deionized water with the above weight ratio into the mixing tank, and after stirring for 3 minutes, reduce the rotating speed of the mixing tank to 400 rpm. Set at 300 revolutions per minute, the indoor temperature of the pulping part is 29°C, put in the cellulose in the above weight ratio, stir for 4 minutes, put in the wetting agent in the above weight ratio, stir for 2 minutes, put in the above weight ratio After stirring for 3 minutes, drop into the ant...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com