A technology of packaging printing and ink, which is applied in the printing field, can solve problems such as polluting the environment, easily volatile toxic and harmful substances, and affecting health, and achieves high environmental protection and economical degree, enhances brilliance and thickness, and reduces pollutants and volatility The effect of pollutants
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] A packaging printing ink, which is composed of the following raw materials in weight percentage: LX-2 resin 15%, acrylic acid 15%, deionized water 15%, paraffin wax 5%, butyl acrylate 5%, ammonia water 15%, urea 2%, gelatin Liquid 1%, glycerin 4%, defoamer 2%, titanium dioxide 1%, D3 resin 10%, solvent 10%.
[0017] The solvent is alcohol, ester solvent.
[0018] A preparation method of packaging printing ink,
[0019] Include the following steps:
[0020] 1) Put acrylic acid and ammonia water into the reaction kettle, then start stirring and slowly add LX-2 resin (add a small amount of pure water during this process), test the pH to 8-8.5, and discharge the material after reaching the standard and filter for use;
[0021] 2) Put butyl acrylate and D3 resin into the reaction kettle and mix, raise the temperature to 45-120°C, start stirring for 15-25 minutes, wait for the mixed solution to stand and become transparent, then slowly add deionized water to adjust the pH t...
Embodiment 2
[0026] A packaging printing ink, which is composed of the following raw materials in weight percentage: 20% LX-2 resin, 10% acrylic acid, 20% deionized water, 1% paraffin, 5% butyl acrylate, 10% ammonia water, 2% urea, gelatin Liquid 2%, glycerin 2%, defoamer 3%, titanium dioxide 3%, D3 resin 12%, solvent 10%.
[0027] The solvent is alcohol, ester solvent.
[0028] A preparation method of packaging printing ink,
[0029] Include the following steps:
[0030] 1) Put acrylic acid and ammonia water into the reaction kettle, then start stirring and slowly add LX-2 resin (add a small amount of pure water during this process), test the pH to 8-8.5, and discharge the material after reaching the standard and filter for use;
[0031] 2) Put butyl acrylate and D3 resin into the reaction kettle and mix, raise the temperature to 45-120°C, start stirring for 15-25 minutes, wait for the mixed solution to stand and become transparent, then slowly add deionized water to adjust the pH to 6...
Embodiment 3
[0036] A packaging printing ink, which is composed of the following raw materials in weight percentage: LX-2 resin 18%, acrylic acid 12%, deionized water 18%, paraffin wax 2%, butyl acrylate 6%, ammonia water 12%, urea 2%, gelatin Liquid 2%, glycerin 2%, defoamer 2%, titanium dioxide 1%, D3 resin 11%, solvent 12%.
[0037] The solvent is alcohol, ester solvent.
[0038] A preparation method of packaging printing ink,
[0039] Include the following steps:
[0040] 1) Put acrylic acid and ammonia water into the reaction kettle, then start stirring and slowly add LX-2 resin (add a small amount of pure water during this process), test the pH to 8-8.5, and discharge the material after reaching the standard and filter for use;
[0041] 2) Put butyl acrylate and D3 resin into the reaction kettle and mix, raise the temperature to 45-120°C, start stirring for 15-25 minutes, wait for the mixed solution to stand and become transparent, then slowly add deionized water to adjust the pH t...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com