Corrosion-resistant rubber pipe material
A rubber tube and corrosion-resistant technology, which is applied in the field of rubber materials, can solve the problems of poor elasticity and tear resistance of reclaimed rubber, difficulty in meeting performance requirements, and harsh environmental conditions in use, so as to achieve excellent product performance and low raw material cost , not easy to aging effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] A corrosion-resistant rubber tube material is characterized in that the components of the raw materials are composed as follows in parts by weight:
[0018] 30 parts of ethylene-propylene rubber, 25 parts of solution-polymerized styrene-butadiene rubber with a styrene content of 26%, 15 parts of SRR-16 reclaimed rubber, 1 part of benzoyl peroxide, 3 parts of NXT silane coupling agent, and 4 parts of nano-graphite , 7 parts of paraffin, 3 parts of talc, 0.7 parts of zinc oxide, 0.6 parts of zinc stearate, 2 parts of epoxy resin, 0.7 parts of disodium hexamethylene-1,6-dithiosulfate, 1.5 parts of titanium dioxide, 1 part of white oil, 0.3 part of antioxidant AT-10, 0.8 part of butylated hydroxytoluene, 2 parts of sulfur.
Embodiment 2
[0020] A corrosion-resistant rubber tube material is characterized in that the components of the raw materials are composed as follows in parts by weight:
[0021] 35 parts of ethylene-propylene rubber, 28 parts of solution-polymerized styrene-butadiene rubber with a styrene content of 27%, 18 parts of SRR-16 reclaimed rubber, 1.5 parts of benzoyl peroxide, 3.5 parts of NXT silane coupling agent, and 6 parts of nano-graphite , 8 parts of paraffin, 3 parts of talc, 0.8 parts of zinc oxide, 0.7 parts of zinc stearate, 3 parts of epoxy resin, 0.8 parts of disodium hexamethylene-1,6-dithiosulfate, 1.6 parts of titanium dioxide, 2 parts of white oil, 0.4 parts of antioxidant AT-10, 0.8 parts of butylated hydroxytoluene, 3 parts of sulfur.
Embodiment 3
[0023] A corrosion-resistant rubber tube material is characterized in that the components of the raw materials are composed as follows in parts by weight:
[0024] 40 parts of ethylene propylene rubber, 28 parts of solution-polymerized styrene-butadiene rubber with a styrene content of 28%, 20 parts of SRR-16 reclaimed rubber, 2 parts of benzoyl peroxide, 4 parts of NXT silane coupling agent, and 7 parts of nano-graphite , 9 parts of paraffin, 4 parts of talc, 0.9 parts of zinc oxide, 0.8 parts of zinc stearate, 4 parts of epoxy resin, 0.9 parts of disodium hexamethylene-1,6-dithiosulfate, 1.8 parts of titanium dioxide, 3 parts of white oil, 0.5 parts of antioxidant AT-10, 0.8 parts of butylated hydroxytoluene, 4 parts of sulfur.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com