A technology of warm-mix asphalt and matrix asphalt, which is applied in building insulation materials, building components, climate change adaptation, etc. It can solve the problem of low-temperature tensile and brittle crack resistance of asphalt mixtures, and reduce the viscosity of modified asphalt at 175°C. Reduce the high-temperature viscosity of asphalt and other problems, and achieve the effects of reducing energy consumption, reducing high-temperature viscosity, and low-temperature viscosity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0033] The mass percentage of warm mix asphalt raw material is:
[0034] Stearic acid: 0.5%;
[0035] Coconut oil fatty acid diethanolamide: 7.5%;
[0036]Base bitumen: 92.0%.
[0037] Add stearic acid and coconut oil fatty acid diethanolamide into the reaction vessel respectively according to the proportion, stir and raise the temperature to 65°C, and the stirring time is 30 minutes, then add it to the base asphalt according to the proportion, the mixing temperature is 147°C, and the stirring time is 50 minutes , made of warm mix asphalt.
Embodiment 2
[0039] The mass percentage of warm mix asphalt raw material is:
[0040] Stearic acid: 7.2%;
[0041] Coconut oil fatty acid diethanolamide: 2.5%;
[0042] Base bitumen: 90.3%.
[0043] Add stearic acid and coconut oil fatty acid diethanolamide into the reaction vessel respectively according to the proportion, stir and heat up to 70°C, and the stirring time is 20 minutes, then add it to the base asphalt according to the proportion, the mixing temperature is 140°C, and the stirring time is 45 minutes , made of warm mix asphalt.
Embodiment 3
[0045] The mass percentage of warm mix asphalt raw material is:
[0046] Stearic acid: 3.6%;
[0047] Coconut oil fatty acid diethanolamide: 1.2%;
[0048] Base bitumen: 95.2%.
[0049] Add stearic acid and coconut oil fatty acid diethanolamide into the reaction vessel respectively according to the proportion, stir and heat up to 85°C, and the stirring time is 25 minutes, then add it to the base asphalt according to the proportion, the mixing temperature is 135°C, and the stirring time is 35 minutes , made of warm mix asphalt.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com