A local uv glue
A topical, adhesive technology, applied in coatings, polyurea/polyurethane coatings, etc., can solve the problems of poor wear resistance, insufficient brightness, transparency, easy to fall off, etc., achieve low cost, prevent gloss loss, high transparency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] A local UV glue is characterized in that it comprises the following raw materials in parts by weight: 60 parts of polypropylene, 8 parts of polyurethane, 27 parts of ethyl 2,4,6-trimethylbenzoylphenyl phosphonate, sulfated castor 10 parts of sesame oil, 2 parts of polydimethylsiloxane, 30 parts of dilauryl thiodipropionate.
[0018] Put polypropylene and polyurethane into the reaction kettle, heat up to 200°C and dissolve completely, start stirring and heat up to 250°C, keep warm for 30 minutes, then add 2,4,6-trimethylbenzoylphenylphosphonic acid ethyl ester, sulfuric acid Melt castor oil, keep warm for 30 minutes, then add polydimethylsiloxane, dilauryl thiodipropionate, keep warm and stir for 20-30 minutes. Apply some UV glue to the carton box. After spraying, put it in an oven at 50°C and bake it with oxygen for 10 days.
Embodiment 2
[0020] A local UV glue, characterized in that it comprises the following raw materials in parts by weight: 70 parts of polypropylene, 8 parts of polystyrene, 27 parts of vinyl ether, 10 parts of lecithin, 2 parts of polymethylphenylsiloxane, 30 parts of tertiary amines.
[0021] Put polypropylene and polystyrene into the reactor, heat up to 200°C and dissolve completely, start stirring and heat up to 250°C, keep warm for 30 minutes, then add vinyl ether and lecithin, keep warm for 30 minutes, then add polymethylbenzene Base siloxane and tertiary amine are kept and stirred for 20-30 minutes, and they are passed out of the pot. Apply some UV glue to the carton box. After spraying, put it in an oven at 50°C and bake it with oxygen for 10 days.
Embodiment 3
[0023] A local UV glue, characterized in that it comprises the following raw materials in parts by weight: 75 parts of polypropylene, 9 parts of polyacrylate, 30 parts of 2-hydroxy-2-methyl-1-phenylacetone, 5 parts of fatty acid glycerides , 7 parts of acrylate, 25 parts of zinc oxide.
[0024] Put polypropylene and polyacrylate into the reactor, heat up to 200°C and dissolve completely, start stirring and heat up to 250°C, keep it warm for 30 minutes, then add 2-hydroxy-2-methyl-1-phenylacetone, fatty acid glyceride , keep warm for 30 minutes, then add acrylic acid ester and zinc oxide, keep warm and stir for 20-30 minutes, and then pass the pot. Apply some UV glue to the carton box. After spraying, put it in an oven at 50°C and bake it with oxygen for 10 days.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com