Embodiment 1
[0047]Nano long-term cooling liquid is Cu-PG nanofluid. That is: add 2% Cu metal nanoparticles to 85.59% PG, 10% DW base liquid, add 2% SDBS dispersant, add 0.1% sodium molybdate, 0.1% sodium benzoate, 0.1% BTA and TTA mixture to In the base liquid, after stirring and dissolving, take it out after ultrasonic vibration for 3 hours, then add 0.01% coloring agent, add 0.1% ammonia water to adjust the pH value to 9.1, and fully stir evenly to form a uniform and stable Cu-PG nanometer Coolant. The thermal conductivity of the fluid is 21% higher than that of the base fluid measured by the transient hot wire method. The percentages of the above raw materials are percentages by weight.
Embodiment 2
[0049] Nano long-term cooling liquid is CuO-GC nanofluid. That is: add 5% CuO metal nanoparticles to 77% GC, 15.97% DW base fluid, add 0.8% SDBS dispersant, add 0.1% sodium molybdate, 0.1% sodium benzoate, 0.1% BTA and TTA mixture to In the base liquid, after stirring and dissolving, put it into ultrasonic vibration for 3 hours and take it out, then add 0.03% coloring agent, add 1% ammonia water to adjust the pH value to 8.5, fully stir evenly, and it becomes CuO-GC nano cooling liquid . The thermal conductivity of the fluid is 30% higher than that of the base fluid. The percentages of the above raw materials are percentages by weight.
Embodiment 3
[0051] Nano long-term coolant is Al2O3-PG, GC nanofluid. That is: add 0.3% Al to 10% PG, 59.49% GC, 29% DW base fluid 2 o 3 For metal nanoparticles, add 0.4% PEG400 dispersant, then stir and dissolve 0.1% sodium molybdate, 0.1% sodium benzoate, 0.1% BTA and TTA mixture in PG, add it to the base liquid, and put it into ultrasonic vibration for 3 Take it out after 1 hour, add 0.01% coloring agent, add 0.5% hydrochloric acid to adjust the pH value to 5.1, stir well and evenly, and serve as PG-GC mixed nano-coolant. The thermal conductivity of the fluid is 19% higher than that of the base fluid. The percentages of the above raw materials are percentages by weight.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
length | aaaaa | aaaaa |
freezing point | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com