Embodiment 1
[0013] Add 5 kg of polyurethane and 6.5 kg of rosin water into the reaction vessel, stir, and fully dissolve; add 0.5 kg of titanium dioxide and 0.2 kg of paraben into the reaction container, heat up to 80 ° C, stir, and react for 60 minutes; Add 1.5 kg of butyl acetate, 1.8 kg of propylene glycol methyl ether acetate, 0.2 kg of sodium polyacrylate, 0.75 kg of sodium dehydroacetate, 0.65 kg of xylene, 0.5 kg of tributyl tin chloride and 0.3 kg of Benzophenone was heated to 110° C., stirred, reacted for 4 hours, and cooled to obtain an anti-yellowing floor coating.
[0014] The construction method of the anti-yellowing floor coating in this example is: polishing with sandpaper → dust removal → smoothing the wall surface → roller coating of a thin layer of anti-yellowing floor coating → drying → roller coating of the second layer of anti-yellowing floor Coating, finishing by roller coating → dry naturally.
[0015] The epoxy resin coating prepared in this embodiment was transfe...
Embodiment 2
[0017] Add 55 kg of polyurethane and 60 kg of rosin water into the reaction container, stir and fully dissolve; add 10 kg of titanium dioxide and 1 kg of paraben into the reaction container, heat up to 90 ° C, stir, and react for 40 minutes; Add 20 kilograms of butyl acetate in the reaction vessel, 15 kilograms of propylene glycol methyl ether acetate, 12 kilograms of sodium polyacrylate, 5 kilograms of sodium dehydroacetate, 5 kilograms of xylene, 10 kilograms of tributyltin chloride and 4 kilograms Benzophenone is heated to 115° C., stirred, reacted for 3.5 hours, and cooled to obtain an anti-yellowing floor coating.
[0018] The construction method of the anti-yellowing floor coating of this embodiment includes the following steps: sanding paper polishing → dust removal → grinding the wall surface → roller coating of a thin layer of anti-yellowing floor coating → drying → roller coating of the second layer of anti-yellowing Change the floor coating, finish by roller coating...
Embodiment 3
[0021] Add 600 kg of polyurethane and 700 kg of rosin water into the reaction vessel, stir, and fully dissolve; add 75 kg of titanium dioxide and 30 kg of paraben into the reaction container, heat up to 85 ° C, stir, and react for 50 minutes; Add 250 kilograms of butyl acetate in the reaction vessel, 200 kilograms of propylene glycol methyl ether acetate, 150 kilograms of sodium polyacrylate, 100 kilograms of sodium dehydroacetate, 800 kilograms of xylene, 75 kilograms of tributyl tin chloride and 50 kilograms Benzophenone is heated to 1120° C., stirred, reacted for 3 hours, and cooled to obtain an anti-yellowing floor coating.
[0022] The construction method of the anti-yellowing floor coating of this embodiment includes the following steps: sanding paper polishing → dust removal → grinding the wall surface → roller coating of a thin layer of anti-yellowing floor coating → drying → roller coating of the second layer of anti-yellowing Change the floor coating, finish by rolle...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com