Embodiment 1
[0016] The protective agent for waste heat boiler in this embodiment includes water, carbohydrazide used to reduce dissolved oxygen in water and promote the formation of a complete and dense protective film on the metal surface, ammonia water used to adjust the pH value, and, An imidazoline quaternary ammonium salt used to form a protective hydrophobic film over the entire metal surface. Among them, the concentration of carbohydrazide is 300-400mg / L, the concentration of imidazoline quaternary ammonium salt is 100-200mg / L; the pH value of the disabled protective agent is 9.5-10.0, which is used to provide an atmosphere for carbon steel surface passivation .
[0017] The shutdown protection method for waste heat boilers in gas turbine power plants in this embodiment is carried out in two steps: the first step is to stop adding phosphate one hour before sliding to stop, and add carbohydrazide until the concentration of carbohydrazide is 300-400mg / L, adjust the pH value to 9.5-...
Embodiment 2
[0020] The composition of the inactive protective agent: the concentration of carbohydrazide is 300-400mg / L, the pH value is 9.5-10.0; the concentration of imidazoline quaternary ammonium salt is 100-200mg / L, the temperature is 100-300°C, and the time is more than 30min.
[0021] The concentration of carbohydrazide is 300-400mg / L (non-toxic. It can reduce the dissolved oxygen in water and has the function of removing oxygen. In addition, it can also reduce high-valent metal oxides to low-valent metal oxides (such as Fe 3 o 4 ), to promote the formation of a complete and dense protective film on the metal surface, so it has a passivation effect); imidazoline quaternary ammonium salt 100-200mg / L (non-toxic. The molecules of the film-forming corrosion inhibitor are based on the relatively large electronegativity The N atom is the center of the polar group (hydrophilic group) and the hydrocarbon group of the non-polar group (hydrophobic group). When they enter the corrosive medium...
Embodiment 3
[0024] The protective agent for waste heat boiler in this embodiment includes water, carbohydrazide used to reduce dissolved oxygen in water and promote the formation of a complete and dense protective film on the metal surface, ammonia water used to adjust the pH value, and, An imidazoline quaternary ammonium salt used to form a hydrophobic protective film on the entire metal surface; wherein, the concentration of carbohydrazide is 300 mg / L, and the concentration of imidazoline quaternary ammonium salt is 120 mg / L; the pH of the deactivated protective agent A value of 10.0 is used to provide an atmosphere for passivation of carbon steel surfaces.
[0025] In this embodiment, the shutdown protection method for waste heat boilers in gas turbine power plants is carried out in two steps: the first step is to stop adding phosphate one hour before the sliding stop, and add carbohydrazide until the concentration of carbohydrazide is 300 mg / L. Use ammonia water to adjust the pH value...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com