Embodiment 1
[0032] First add 500ml of distilled water to container 1, heat it to 80°C, then add 15g of Span 60, 10g of Tween 20 and 100g of vegetable white oil in sequence, and stir at high speed. After complete emulsification, add 80g of paraffin and 20g of ammonium lauryl sulfate and 10g of simethicone, and stir at high speed until completely emulsified.
[0033] Mix nano-zinc oxide, nano-titanium dioxide, nano-strontium oxide, nano-tourmaline powder, tea extract, and aloe extract in a weight ratio of 0.5:0.1:0.1:1:5:5 and stir until uniformly dispersed to form a solid Active ingredients 1.
[0034] Add 200ml of distilled water to container 2 and heat it to 40°C, then add 10g of Span 60 and 20g of Tween 20 in turn to make an emulsion.
[0035] Add 50g of solid active ingredient 1 into container 2 and keep stirring to make a nano-metal dispersion.
[0036] Finally, pour the nano-metal dispersion in container 2 into container 1 and keep stirring until it is evenly dispersed to make liqu...
Embodiment 2
[0038] First add 300ml of deionized water to container 1, heat it to 100°C, then add 15g of Span 20, 10g of Tween 40, 50g of animal white oil, and 5g of 1618 alcohol in sequence, and stir at high speed. After complete emulsification, add 50g of beeswax or wormwood Wax, 10g simethicone, 100ml polyethylene glycol, 20ml polyethyleneimine, stir until completely emulsified.
[0039] Mix nano-zinc oxide, nano-titanium dioxide, nano-strontium oxide, nano-tourmaline powder, tea extract, and aloe extract according to the weight ratio of 5:2:3:5:5:5 and stir until uniformly dispersed to form a solid Active ingredients 1.
[0040] Add 300ml of water to container 2 and heat it to 60°C, add 15g of Span 20, 15g of Tween 40, and 20ml of OP-10 in sequence and keep stirring to make an emulsified solution, then add 50g of solid active ingredient 1 and stir at a high speed to make a nano metal dispersion.
[0041] Add the emulsion in container 1 to container 2 and stir evenly to make liquid em...
Embodiment 3
[0043] First add 100ml of water and 50g of glycerin to container 1 and heat to 90°C, then add 15g of Span 80, 10g of Tween 60, 50g of vegetable white oil, 5g of 1618 alcohol, and stir at high speed. After complete emulsification, add 60g of palm Wax, 30g laurylamide and 10g simethicone, and stir at high speed until completely emulsified.
[0044] Add 50ml of water to container 2 and heat to 50°C, then add 5g of Span 80 and 6g of Tween 60 in turn to make an emulsion.
[0045] Mix nano-zinc oxide, nano-titanium dioxide, nano-strontium oxide, nano-tourmaline powder, tea extract, and aloe extract according to the weight ratio of 2:0.5:0.3:3:5:5 and stir until uniformly dispersed to form a solid Active ingredients 1.
[0046] Then gradually add 10 g of solid active ingredient 1 into container 2 and keep stirring to prepare nano metal dispersion.
[0047] Finally, pour the nano-metal dispersion in container 2 into container 1 gradually and stir until it is evenly dispersed and coo...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com