A technology of tourmaline and activator, applied in the petroleum industry, fuel, liquid carbon-containing fuel, etc., can solve the problems of unstable performance, secondary pollution parts, high cost, etc., to improve fuel combustion efficiency and infrared radiation rate , The effect of enhancing the conductivity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] 1, the preparation method of above-mentioned tourmaline oil activator, comprises the following steps:
[0029] (1) Mix tourmaline mineral powder, Fe-Mn-Cu spinel ferrite, NaF and CaF 2 Grind them into nano-scale powders respectively, compound tourmaline nano-powder and spinel ferrite nano-powder according to the ratio of 87:9:4, add NaF and CaF 2 Nano powders are mixed and sintered at 500°C for 1 hour in a reducing atmosphere to obtain a solid mixture A;
[0030] (2) Mix 2% sodium dodecylbenzene sulfonate and 5% water, stir for 10 minutes to make it evenly mixed, and get mixed solution B;
[0031] (3) Put the mixture A in the step (1) into the mixed liquid B in the step (2), the input amount of the mixture A is 1% of the total amount of solid-liquid mixing, stir for 20 minutes to completely disperse it, control the temperature as 5°C below the flash point of fuel.
[0032] 2. The tourmaline fuel activator prepared above is directly added to the automobile fuel activa...
Embodiment 2
[0035] 1, the preparation method of above-mentioned tourmaline oil activator, comprises the following steps:
[0036] (1) Mix tourmaline mineral powder, Fe-Mn-Cu spinel ferrite, NaF and CaF 2 Grind them into nano-scale powders respectively, compound tourmaline nano-powder and spinel ferrite nano-powder according to the ratio of 93:5:2, add NaF and CaF 2 Nano-powders are mixed and sintered at 600°C for 3 hours in a reducing atmosphere to obtain a solid mixture A;
[0037] (2) Mix 20% coconut oleic acid alkanolamide and 50% water, stir for 10 minutes to make it evenly mixed, and get the mixed liquid B;
[0038] (3) Put the mixture A in the step (1) into the mixed liquid B in the step (2), the input amount of the mixture A is 3% of the total amount of solid-liquid mixing, stir for 20 minutes to completely disperse it, control the temperature as 5°C below the flash point of fuel.
[0039] 2. The tourmaline fuel activator prepared above is directly added to the automobile fuel act...
Embodiment 3
[0042] 1, the preparation method of above-mentioned tourmaline oil activator, comprises the following steps:
[0043] (1) Mix tourmaline mineral powder, Fe-Mn-Cu spinel ferrite, NaF and CaF 2 Grind them into nano-scale powders respectively, compound tourmaline nano-powder and spinel ferrite nano-powder according to the ratio of 90:7:3, add NaF and CaF 2 Nano-powders are mixed and sintered at 550°C for 2 hours in a reducing atmosphere to obtain a solid mixture A;
[0044] (2) Mix 30% monoglyceride and 98% water, stir for 10 minutes to make it evenly mixed, and get mixed liquid B;
[0045] (3) Put the mixture A in the step (1) into the mixed liquid B in the step (2), the input amount of the mixture A is 5% of the total amount of solid-liquid mixing, stir for 20 minutes to completely disperse it, control the temperature as 5°C below the flash point of fuel.
[0046] 2. The tourmaline fuel activator prepared above is directly added to the automobile fuel activator by 0.02% of t...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com