Method for tanning leather without pickling
A tanning and pickling technology, which is applied in small raw hides/large raw hides/leather/fur treatment, small raw hides/large raw hides/leather hides/fur chemical treatment, chemical treatment before tanning, etc., to reduce pickling operations and avoid ammonium Salt contamination, the effect of strengthening the softening effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0029] Embodiment 1: cow head layer tanning process
[0030] 1. Deliming and softening: According to product characteristics, low-temperature softening enzymes are used for softening treatment. The dosage of softening enzymes is 0.8-1.5% of the tare weight (0-0.5% higher than that of conventional low-temperature softening enzymes). The rotation) time is 60-90 minutes (20-60 minutes longer than the softening time of conventional low-temperature softening enzymes). Requirements: The temperature is normal temperature, the deashing must be thorough, and the pH value of the bath liquid is measured to be 8.0 to 8.5. The rotational speed of the rotating drum is the same as that required by the existing process.
[0031] 2. Chrome tanning without pickling:
[0032] Add 30% of normal temperature water (about 25°C) into the tanning drum, and then proceed sequentially:
[0033] Add pickling oil 0.3~0.5% and rotate for 20min
[0034] Add SF-1 2.5~3.5% and rotate for 60min
[0035] Ad...
Embodiment 2
[0041] Embodiment 2: cattle two-layer tanning process
[0042] 1. Deliming and softening: According to product characteristics, low-temperature softening enzyme is used for softening treatment. The dosage of softening enzyme is 0.6-1.2% of the tare weight (0-0.5% higher than the conventional dosage), and the dosage of degreasing agent is tare weight. 0.3 to 0.8% of the degreasing operation of conventional cowhide processing is carried out in the stage of water immersion, liming or retanning, while the non-pickling chrome tanning technology is used for the tanning of cow split leather, because the split leather has a high oil content, In order to avoid the presence of grease at high pH values, an additional step is added after the addition of non-pickling chrome tanning agents to produce chrome soaps). The rotation time of the softening drum is 60-90 minutes (30-60 minutes longer than the conventional time). Requirements: The temperature is normal temperature, the deashing mus...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com