Real stone paint and preparation method thereof
A technology of real stone paint and dispersant, applied in the direction of coating, etc., can solve the problems of poor flexibility, difficult manual cleaning, insufficient anti-fouling ability of real stone paint, etc., and achieve the effect of excellent flexibility
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0032] A real stone paint prepared from the following raw materials: 80.0kg of water, 3.0kg of ethylene glycol, 10.0kg of BYK-156 dispersant, 1.0kg of Deqian W-18 wetting agent, Dow ER-30M hydroxyethyl Base cellulose 4.0kg, Dow AMP-95PH regulator 4.0kg, silica sol 10.0kg, BASF SC138 elastic emulsion 30.0kg, BASF 296D-S styrene-acrylic emulsion 90.0kg, 20-40 mesh natural colored sand fine sand 60.0kg, 40-80 mesh natural colored sand medium sand 240.0kg, 80-120 mesh natural colored sand coarse sand 400.0kg, real stone varnish rock flakes of various colors 50.0kg, Eastman Texanol film-forming aid 10.0kg, BYK-024 defoamer 4.0kg, Deqian MB-11 preservative 4.0kg.
[0033] The preparation method of the real stone paint provided by the present embodiment 1 may further comprise the steps:
[0034] 1. In the real stone paint production equipment, add water 80.0kg, ethylene glycol 3.0kg, BYK-156 dispersant 10.0kg, Deqian W-18 wetting agent 1.0kg and Dow ER-30M hydroxyethyl Cellulose 4....
Embodiment 2
[0039] A real stone paint prepared from the following raw materials: 120.0kg of water, 17.0kg of ethylene glycol, 1.0kg of Dow H-30A dispersant, 0.2kg of BYK-310 wetting agent, and 0.2kg of Dow ER-30M hydroxyethyl Base cellulose 0.2kg, Deqian DMAE water-based amine neutralizer 0.2kg, silica sol 40.0kg, BASF SC138 elastic emulsion 50.0kg, BASF 296D-S styrene-acrylic emulsion 20.0kg, 20-40 mesh natural colored sand fine sand 40.0kg , 160.0kg medium sand of 40-80 mesh natural colored sand, 480.0kg natural colored sand coarse sand of 80-120 mesh, 70.0kg rock flakes of various colors, Eastman Texanol film-forming aid 1.0kg, BYK-033 defoaming agent Antiseptic 0.2kg, Deqian MB-16 preservative 0.2kg.
[0040] The preparation method of the real stone paint provided by the present embodiment 2 may further comprise the steps:
[0041] 1. In the real stone paint production equipment, add 120.0kg of water, 17.0kg of ethylene glycol, 1.0kg of Dow H-30A dispersant, 0.2kg of BYK-310 wetting ag...
Embodiment 3
[0046] A real stone paint prepared from the following raw materials: 106.5kg of water, 10.0kg of ethylene glycol, 5.0kg of Godix P-90 dispersant, 0.5kg of Dow X-405 wetting agent, 0.5kg of Dow ER-30M hydroxyl Ethyl cellulose 2.0kg, camine328 multifunctional additive 2.0kg, silica sol 25kg, BASF SC138 elastic emulsion 40.0kg, BASF 296D-S styrene-acrylic emulsion 50.0g, 20~40 mesh natural colored sand fine sand 50.0kg, 40~ 80 mesh natural colored sand medium sand 200.0kg, 80~120 mesh natural colored sand coarse sand 440.0kg, real stone varnish rock flakes of various colors 60.0kg, Eastman Texanol film-forming aid 5.0kg, Nopco SN-NXZ defoamer 2.0 kg, Rohm and Haas LXE preservative 2.0kg.
[0047] The preparation method of the real stone paint provided by the present embodiment 3 may further comprise the steps:
[0048] 1. In the genuine stone paint production equipment, add water 106.5kg, ethylene glycol 10.0kg, Godix P-90 dispersant 5.0kg, Dow X-405 wetting agent 0.5kg and Dow ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com