Flame-proof treatment method of real silk fabrics by biological enzyme method
A technology for flame-retardant finishing of real silk fabrics, applied in biochemical fiber treatment, fiber treatment, animal fiber, etc., can solve the problems of large fiber damage, high energy consumption, and environmental pollution, and achieve improved flame-retardant effect, low energy consumption, The effect of avoiding silk fiber damage
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
specific Embodiment
[0022] Using tyrosinase to catalyze the oxidation of silk fibroin, grafting organophosphorus flame retardants with primary amino groups on the surface of real silk fibers, and improving the flame retardancy of real silk fabrics. The specific examples are as follows:
Embodiment 1
[0023] Implementation 1: The silk fabric selected in this implementation is electric spinning, and the treatment with tyrosinase and organic phosphorus flame retardant is carried out step by step in the same bath.
[0024] (1) Tyrosinase treatment: real silk fabrics were immersed in tyrosinase solution for 4 hours, wherein tyrosinase 25U / g fabric, penetrant 0.5g / L solution, temperature 30°C, pH=7.0.
[0025] (2) Grafting with organophosphorus flame retardant: the silk was treated with tyrosinase for 4 hours, then sodium alendronate (10 g / L) was added, and the treatment was continued for 4 hours at a temperature of 30° C. and pH=7.0.
[0026] (3) Post-treatment: After the enzyme treatment, the silk fabric was fully washed with deionized water, and dried at 60° C. for later use.
[0027] Sample 1: a blank sample impregnated with alendronate sodium;
[0028] Sample 2: Sample treated with tyrosinase and alendronate sodium;
[0029] After the above process treatment, the limiting...
Embodiment 2
[0030] Implementation 2: The silk fabric selected in this implementation is crepe de chine, and the treatment with tyrosinase and organic phosphorus flame retardant is carried out by two-bath method respectively.
[0031] (1) Silk pretreatment: pre-swell silk fabrics with EDTA and urea solution, including 0.25g / L EDTA, 0.25g / L urea, 0.25g / L penetrant, temperature 40°C, treatment time 1 hour, silk The fabric is fully washed.
[0032] (2) Tyrosinase treatment: soak the pretreated silk fabric in tyrosinase solution for 6 hours, wherein tyrosinase 50U / g fabric, penetrant 0.25g / L solution, temperature 30°C, pH =7.0.
[0033] (3) Flame retardant grafting: take out the real silk fabric after tyrosinase treatment, and treat it in alendronate sodium solution for 6 hours, wherein alendronate sodium 15g / L, temperature 30 ℃, pH=7.0 .
[0034] (4) Post-treatment: After the enzyme treatment, the silk fabric was fully washed with deionized water, and dried at 60° C. for later use.
[003...
PUM
Property | Measurement | Unit |
---|---|---|
limiting oxygen index | aaaaa | aaaaa |
limiting oxygen index | aaaaa | aaaaa |
limiting oxygen index | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.