Embodiment 1
[0032] Add high hydrogen-containing silicone oil, D4, hexamethyldisilazane, and ammonia water into a reaction kettle equipped with a stirrer, a reflux condenser, and a thermometer at a ratio of 10:0.5:0.1:0.1, stir, and heat up to 60°C After reacting for 3 hours, add 80% sulfamic acid of the above-mentioned ammonia water, continue to stir for 2 hours, carry out suction filtration, distillation, and remove low boilers to obtain low-hydrogen silicone oil with proper hydrogen content;
[0033] Add low-hydrogen silicone oil and D4 into the reaction kettle equipped with stirrer, reflux condenser and thermometer in sequence at a ratio of 10:2, and pass N 2 Stir, heat up to 100°C, add zinc oxide, continue to stir, and react at a constant temperature of 90°C for 2 hours, the reaction solution becomes turbid and clear;
[0034] Then add aminopropyl trimethylsilane and allyl polyoxyethylene ether into the reaction kettle at a ratio of 1; Tetraethylenetriamine was reacted for 4 hours, a...
Embodiment 2
[0044] Add high hydrogen-containing silicone oil, DMC, hexamethyldisilazane, and ammonia water in a ratio of 10:0.5:0.1:0.1 into a reaction kettle equipped with a stirrer, a reflux condenser, and a thermometer, stir, and heat up to 60°C After reacting for 4 hours, add sulfamic acid in an amount of 80% of the above-mentioned weakly basic inorganic substance, continue to stir for 2 hours, then carry out suction filtration, distillation, and removal of low boilers to obtain low-hydrogen silicone oil with an appropriate hydrogen content;
[0045] Add low-hydrogen silicone oil and D4 into the reaction kettle equipped with stirrer, reflux condenser and thermometer in sequence at a ratio of 10:2, and pass N 2 Stir, heat up to 100°C, add zinc oxide, continue to stir, and react at a constant temperature of 90°C for 2 hours, the reaction solution becomes turbid and clear;
[0046] Add aminopropyl trimethylsilane and allyl polyoxyethylene ether into the reaction kettle in turn at a ratio...
PUM
Property | Measurement | Unit |
---|---|---|
Viscosity | aaaaa | aaaaa |
Viscosity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com