A technology for condensate oil in alpine regions, applied in the petroleum industry, hydrocarbon distillation, liquid carbon-containing fuels, etc., can solve the problem of not being able to completely replace, and achieve the effect of improving the utilization value, increasing the output, and having sufficient raw materials
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0063] Special additives are prepared by the following methods, please refer to image 3 , the special additive preparation method comprises the following steps:
[0064] Step S300, placing the weighed fatty alcohol polyoxyethylene ether and oleic acid in a reactor with a stirring device under ambient pressure, wherein the ambient pressure refers to the natural atmospheric pressure in the area where the production facility is located;
[0065] Step S301, under stirring, slowly add naphthenate, petroleum ether and core additives, while keeping the temperature of the mixed material at 30-80°C, in which fatty alcohol polyoxyethylene ether, oleic acid, naphthenate, petroleum The weight percent of ether, core additive is:
[0066] Fatty alcohol polyoxyethylene ether 10-30%;
[0067] Oleic acid 10-20%;
[0068] Naphthenate 20-25%;
[0069] Petroleum ether 10-15%;
[0070] Core additives 10-40%;
[0071] In step S302, after all the materials are added, the heat preservation and...
Embodiment 1
[0084] The components of special additives and the percentage by weight of each component are:
[0085]
[0086]
[0087] Described core additive, its component and the weight percent of each component are:
[0088]
[0089] The special additive preparation method is as follows:
[0090] Under ambient pressure, place the weighed fatty alcohol polyoxyethylene ether and oleic acid in a reactor with a stirring device; under stirring, slowly add sodium naphthenate, petroleum ether and core additives while maintaining The temperature of the mixed material is 70°C; after adding all the materials, continue to keep warm and stir for 60 minutes, and discharge the material to obtain the special additive.
[0091] The preparation method of described core additive is as follows:
[0092] Under ambient pressure, place the weighed rapeseed sulfonated oil in a reaction kettle with a stirring device; under stirring, slowly add ferrocene, potassium chlorate, sodium sulfonate, diethy...
Embodiment 2
[0094] The components of special additives and the percentage by weight of each component are:
[0095]
[0096] Described core additive, its component and the weight percent of each component are:
[0097]
[0098] The preparation method of special additive is as follows:
[0099] Under ambient pressure, place the weighed fatty alcohol polyoxyethylene ether and oleic acid in a reactor with a stirring device; under stirring, slowly add barium naphthenate, petroleum ether and core additives, while maintaining The temperature of the mixed material is 70°C; after all the materials are added, continue to keep warm and stir for 40 minutes, and discharge the material to obtain the special additive.
[0100] The preparation method of described core additive is as follows:
[0101] Under ambient pressure, place the weighed linseed sulfonated oil in a reaction kettle with a stirring device; under stirring, slowly add ferrocene, potassium chlorate, barium sulfonate, triethylene ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com