Air purifier and preparation method thereof
An air purifier and equipment technology, which is applied in the field of air purifier and its preparation, can solve the problems of inability to precisely detect the requirements of air purity and dryness, and achieve the effect of meeting the requirements of dryness and high purification degree.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] Comprise the following steps: a, calcium sulfate is ground with pulverizer, and sieve out too big or too small particle, get the calcium sulfate 300g that diameter is 0.8mm-2mm and dye it with 100g cobalt chloride, require dyeing evenly, The dyeing method is as follows: the dyeing is to dissolve cobalt chloride in water, put it into a watering can, put calcium sulfate into the drum, and spray the cobalt chloride solution such as calcium sulfate for dyeing while the drum is rotating. Bake the dyed calcium sulfate in an oven at 300°C for 6 hours, then seal it and place it at room temperature; b, take 100g of activated carbon and bake it in an oven at 240°C for 3 hours, then seal it and place it at room temperature; C 1. Mix the materials obtained in step a and step b evenly to obtain the air purifier of the present invention.
Embodiment 2
[0017] Comprise the following steps: a, calcium sulfate is ground with pulverizer, and sieve out too big or too small particle, get the calcium sulfate 254g after pulverizing and dye it with 85g cobalt chloride, require dyeing evenly, dyeing method is: Dyeing is to first dissolve cobalt chloride in water, put it into a watering can, put calcium sulfate into the drum, and spray the cobalt chloride solution such as calcium sulfate for dyeing while the drum is rotating. Bake the dyed calcium sulfate in an oven at 300°C for 6 hours, then seal it and place it at room temperature; b, take 85g of activated carbon and bake it in an oven at 240°C for 3 hours, then seal it and place it at room temperature; C 1. Mix the materials obtained in step a and step b evenly to obtain the air purifier of the present invention.
Embodiment 3
[0019] Comprise the following steps: a, calcium sulfate is ground with pulverizer, and sieve out too big or too small particle, get the calcium sulfate 314g after pulverizing and dye it with 105g cobalt chloride, require dyeing evenly, dyeing method is: Dyeing is to first dissolve cobalt chloride in water, put it into a watering can, put calcium sulfate into the drum, and spray the cobalt chloride solution such as calcium sulfate for dyeing while the drum is rotating. Bake the dyed calcium sulfate in an oven at 300°C for 6 hours, then seal it and place it at room temperature; b, take 105g of activated carbon and bake it in an oven at 240°C for 3 hours, then seal it and place it at room temperature; C 1. Mix the materials obtained in step a and step b evenly to obtain the air purifier of the present invention.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com