Manufacture method of synergic type nitrogenous fertilizer with slow release and loss control effect
A manufacturing method, slow-release technology, applied in the direction of fertilization device, fertilizer mixture, application, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0091] Synergistic urea production with slow release and loss control:
[0092] 1. Composition and formula of slow release and loss control materials:
[0093] Oyster shell powder: chitosan: humic acid: polyacrylamide: organic acid chelated titanium: urea peroxide is composed in a weight ratio of 100:1.0:4.0:3.0:0.10:0.10.
[0094] 2. Microwave-assisted modification of chitosan to manufacture modified oyster shell powder adsorbent:
[0095] Dissolve 10kg of chitosan in 1000kg of aqueous solution containing 5% organic acid to prepare a 1.0% concentration of chitosan solution.
[0096] Soak 1000kg of oyster shells with a fineness greater than or equal to 100 mesh in the chitosan solution for 60 minutes.
[0097] Place the mixture of oyster shell powder and chitosan solution in batches in a polyvinyl fluoride container, and irradiate the oyster shell powder in a microwave field with a microwave operating frequency of 2450 MHz and a microwave power of 10 KW for 15 minutes to 30 ...
Embodiment 2
[0109] Manufacture of synergistic ammonium sulfate fertilizer with slow release and loss control effects:
[0110] 1. Composition and formula of slow release and loss control materials:
[0111] Oyster shell powder: chitosan: humic acid: polyacrylamide: organic acid chelated titanium: urea peroxide is composed in a weight ratio of 100:0.5:3.0:2.5:0.05:0.05.
[0112] 2. Microwave-assisted modification of chitosan to manufacture modified oyster shell powder adsorbent:
[0113] Dissolve 5kg of chitosan in 1000kg of aqueous solution containing 5% organic acid to prepare a 0.5% concentration of chitosan solution.
[0114] Soak 1000kg of oyster shells with a fineness greater than or equal to 100 mesh in the chitosan solution for 60 minutes.
[0115] Place the mixture of oyster shell powder and chitosan solution in batches in polyvinyl fluoride containers, and irradiate the oyster shell powder in a microwave field with a microwave operating frequency of 2450MHz and a microwave powe...
Embodiment 3
[0127] Manufacture of synergistic ammonium bicarbonate fertilizer with slow release and loss control effects:
[0128] 1. Composition and formula of slow release and loss control materials:
[0129] Oyster shell powder: chitosan: humic acid: polyacrylamide: organic acid chelated titanium: urea peroxide is composed in a weight ratio of 100:2.0:5.0:4.0:0.15:0.15.
[0130] 2. Microwave-assisted modification of chitosan to manufacture modified oyster shell powder adsorbent:
[0131] Dissolve 5kg of chitosan in 2000kg of aqueous solution containing 5% organic acid to prepare a 1.0% concentration of chitosan solution.
[0132] Soak 1000kg of oyster shells with a fineness greater than or equal to 100 mesh in the chitosan solution for 60 minutes.
[0133] Place the mixture of oyster shell powder and chitosan solution in batches in a polyvinyl fluoride container, and irradiate the oyster shell powder in a microwave field with a microwave operating frequency of 2450 MHz and a microwav...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com